A crystal structure (left) and a visual model of its spin helix (right). Image: McCormick School of Engineering, Northwestern University.As our lives become increasingly intertwined with technology – whether supporting communication while working remotely or streaming our favorite show – so too does our reliance on the data these devices create. Data centers supporting these technology ecosystems produce a significant carbon footprint – and consume 200 terawatt hours of energy each year, greater than the annual energy consumption of Iran. To balance ecological concerns yet meet growing demand, advances in microelectronic processors – the backbone of many Internet of Things (IoT) devices and data hubs – must be efficient and environmentally friendly.
Materials scientists at Northwestern University have developed new design principles that could help spur development of future quantum materials for advancing IoT devices and other resource-intensive technologies while limiting ecological damage. The scientists describe these design principles in a paper in Matter.
"New path-breaking materials and computing paradigms are required to make data centers more energy-lean in the future," said James Rondinelli, professor of materials science and engineering and professor in materials and manufacturing at Northwestern University's McCormick School of Engineering, who led the research.
This study marks an important step in Rondinelli's efforts to create new materials that are non-volatile, energy efficient and generate less heat – important requirements for future ultrafast, low-power electronics and quantum computers that can help meet the world's growing demand for data.
Rather than certain classes of semiconductors using the electron's charge in transistors to power computing, solid-state spin-based materials utilize the electron's spin and have the potential to support low-energy memory devices. In particular, materials with a high-quality persistent spin texture (PST) can exhibit a long-lived persistent spin helix (PSH), which can be used to track or control the spin-based information in a transistor.
Although many spin-based materials already encode information using spins, this information can be corrupted as the spins propagate in the active portion of the transistor. The researchers' novel PST protects that spin information in helix form, making it a potential platform where ultralow energy and ultrafast spin-based logic and memory devices operate.
Using quantum-mechanical models and computational methods, the researchers developed a framework to identify and assess the spin textures in a group of non-centrosymmetric crystalline materials. The ability to control and optimize the spin lifetimes and transport properties in these materials is vital to realizing the future of quantum microelectronic devices that operate with low energy consumption.
"The limiting characteristic of spin-based computing is the difficulty in attaining both long-lived and fully controllable spins from conventional semiconductor and magnetic materials," Rondinelli said. "Our study will help future theoretical and experimental efforts aimed at controlling spins in otherwise non-magnetic materials to meet future scaling and economic demands."
Rondinelli's framework used microscopic effective models and group theory to identify three materials design criteria that would produce useful spin textures. These criteria are: carrier density, the number of electrons propagating through an effective magnetic field; Rashba anisotropy, the ratio between intrinsic spin-orbit coupling parameters of the materials; and momentum space occupation, the PST region active in the electronic band structure. These features were then assessed using quantum-mechanical simulations to discover high-performing PSHs in a range of oxide-based materials.
The researchers used these principles, along with numerical solutions to a series of differential spin-diffusion equations, to assess the spin texture of each material and predict the spin lifetimes for the helix in the strong spin-orbit coupling limit. They also found they could adjust and improve the PST performance using atomic distortions at the picoscale. This allowed them to determine an optimal PST material, Sr3Hf2O7, which showed a substantially longer spin lifetime for the helix than any previously reported material.
"Our approach provides a unique chemistry-agnostic strategy to discover, identify, and assess symmetry-protected persistent spin textures in quantum materials using intrinsic and extrinsic criteria," Rondinelli said. "We proposed a way to expand the number of space groups hosting a PST, which may serve as a reservoir from which to design future PST materials, and found yet another use for ferroelectric oxides – compounds with a spontaneous electrical polarization. Our work also will help guide experimental efforts aimed at implementing the materials in real device structures."
This story is adapted from material from Northwestern University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.