This illustration shows a battery's cathode undergoing phase transition from iron phosphate (FP) to lithium iron phosphate (LFP) during charging. Simulations by Rice University scientists showed that adding defects – distortions in the crystal lattice – could help batteries charge faster. Image: Kaiqi Yang/Rice University.Scientists at Rice University's Brown School of Engineering have discovered that placing specific defects in the crystalline lattice of lithium iron phosphate-based cathodes, as used in lithium-ion batteries, broadens the avenues through which lithium ions travel. Their theoretical calculations could improve the performance of these cathodes by up to two orders of magnitude and point the way to similar improvements in other types of batteries.
These defects, known as antisites, are formed when atoms are placed at the wrong positions on the lattice – that is, when iron atoms sit on the sites that should be occupied by lithium atoms. Antisite defects impede lithium movement inside the crystal lattice and are usually considered detrimental to battery performance.
In the case of lithium iron phosphate, however, the Rice researchers discovered that antisites create detours within the cathode that allow lithium ions to reach the reaction front over a wider surface, which helps improve the charge and discharge rate of the batteries. The researchers report their findings in a paper in npj Computational Materials.
According to Rice materials scientist Ming Tang, lithium iron phosphate is a widely used cathode material for lithium-ion batteries and also serves as a good model system for studying the physics underlying the battery cycling process. Tang carried out this research with Rice alumnus Liang Hong, now a researcher at MathWorks, and graduate student Kaiqi Yang.
Upon lithium insertion, the cathode changes from a lithium-poor phase to a lithium-rich one. When the surface reaction kinetics are sluggish, lithium can only be inserted into lithium iron phosphate within a narrow surface region around the phase boundary – the ‘road’ – a phenomenon that limits the speed at which the battery can recharge.
"If there are no defects, lithium can only enter this small region right around the phase boundary," Tang explained. "However, antisite defects can make lithium insertion take place more uniformly across the surface, and so the boundary would move faster and the battery would charge faster.
"If you force the defect-free cathode to be charged fast by applying a large voltage, there will be a very high local lithium flux at the surface and this can cause damage to the cathode. This problem can be solved by using defects to spread the flux over the entire cathode surface."
Annealing the material – heating without burning it – can be used to control the concentration of defects. Tang said that these defects would also allow larger cathode particles to be used, helping to improve energy density and reduce surface degradation.
"An interesting prediction of the model is that this optimal defect configuration depends on the shape of the particles," he said, "We saw that facets of a certain orientation could make the detours more effective in transporting lithium ions. Therefore, you will want to have more of these facets exposed on the cathode surface."
According to Tang, the model could be applied as a general strategy to improve phase-changing battery compounds. "For structural materials like steel and ceramics, people play with defects all the time to make materials stronger," he said. "But we haven't talked much about using defects to make better battery materials. Usually, people see defects as annoyances to be eliminated.
"But we think we can turn defects into friends, not enemies, for better energy storage."
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.