Materials scientists at Argonne National Laboratory synthesized these single crystals of a metallic trilayer nickelate compound via a high-pressure crystal growth process. Photo: Argonne National Laboratory.A team of researchers at the US Department of Energy's (DOE) Argonne National Laboratory has identified a nickel oxide compound as an unconventional but promising candidate material for high-temperature superconductivity. The team successfully synthesized single crystals of a metallic trilayer nickelate compound, a feat the researchers believe to be a first.
This nickel oxide compound does not actually superconduct, said John Mitchell, associate director of the laboratory's Materials Science Division, who led the project, which combined crystal growth, X-ray spectroscopy and computational theory. But, he added, "It's poised for superconductivity in a way not found in other nickel oxides. We're very hopeful that all we have to do now is find the right electron concentration." Mitchell and seven co-authors report their results in a paper in Nature Physics.
Superconducting materials are technologically important because electricity flows through them without resistance. High-temperature superconductors could lead to faster, more efficient electronic devices, power grids that can transmit electricity without energy loss and ultra-fast levitating trains that ride frictionless magnets instead of rails.
Only low-temperature superconductivity seemed possible before 1986, but materials that superconduct at low temperatures are impractical because they must first be cooled to hundreds of degrees below zero. In 1986, however, the discovery of high-temperature superconductivity in copper oxide compounds known as cuprates suggested new technological potential for the phenomenon.
But after three decades of ensuing research, exactly how cuprate superconductivity works remains a defining problem in the field. One approach to solving this problem has been to study compounds that have similar crystal, magnetic and electronic structures to the cuprates.
Nickel-based oxides – nickelates – have long been considered as potential cuprate analogs because nickel sits immediately adjacent to copper in the periodic table. Thus far, Mitchell noted, "that's been an unsuccessful quest". As he and his co-authors noted in their Nature Physics paper: "None of these analogs have been superconducting, and few are even metallic."
The nickelate that the Argonne team has created is a quasi-two-dimensional trilayer compound, meaning it comprises three layers of nickel oxide that are separated by spacer layers of praseodymium oxide. "Thus it looks more two-dimensional than three-dimensional, structurally and electronically," Mitchell said.
This nickelate shares its quasi-two-dimensional trilayer structure with a similar compound containing lanthanum rather than praseodymium. But the lanthanum analog is non-metallic and adopts a so-called ‘charge-stripe’ phase, an electronic property that makes the material an insulator, the opposite of a superconductor.
"For some yet-unknown reason, the praseodymium system does not form these stripes," Mitchell said. "It remains metallic and so is certainly the more likely candidate for superconductivity."
Argonne is one of a few laboratories in the world where the compound could be created, thanks to the special abilities of the Materials Science Division's high-pressure optical-image floating zone furnace. This furnace can attain pressures of 150 atmospheres (equivalent to the crushing pressures found at oceanic depths of nearly 5000 feet) and temperatures of approximately 2000°C, just the conditions needed to grow the crystals.
"We didn't know for sure we could make these materials," said Argonne postdoctoral researcher Junjie Zhang, first author on the study. But they were able to grow nickelate crystals measuring a few millimeters in diameter (a small fraction of an inch).
The research team verified that the electronic structure of the nickelate resembles that of cuprate materials by taking X-ray absorption spectroscopy measurements at the Advanced Photon Source, a DOE Office of Science User Facility, and by performing density functional theory calculations. Materials scientists use density functional theory to investigate the electronic properties of condensed matter systems.
"I've spent my entire career not making high-temperature superconductors," Mitchell joked. But that could change in the next phase of his team's research: attempting to induce superconductivity in their nickelate material using a chemical process called electron doping, in which impurities are deliberately added to a material to influence its properties.
This story is adapted from material from Argonne National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.