Engineering stronger grain boundaries in perovskite materials can help to channel ions and oxygen along those boundaries, preventing them from entering the crystal grains. Image: NC State.Researchers have discovered that channeling ions into defined pathways in perovskite materials improves the stability and operational performance of perovskite solar cells. This finding paves the way for a new generation of lighter, more flexible and more efficient solar-cell technologies suitable for practical use.
Perovskite materials, which are defined by their crystalline structure, are better at absorbing light than silicon. That means perovskite solar cells can be thinner and lighter than silicon solar cells without sacrificing the cell’s ability to convert light into electricity.
“That opens the door to a host of new technologies, such as flexible, lightweight solar cells, or layered solar cells (known as tandems) that can be far more efficient than the solar-harvesting technology used today in so-called solar farms,” says Aram Amassian, a professor of materials science and engineering at North Carolina State University (NC State) and corresponding author of a paper on this discovery in Nature Materials. “There’s interest in integrating perovskite materials into silicon solar-cell technologies, which would improve their efficiency from 25% to 40% while also making use of existing infrastructure.”
However, working with perovskite materials poses a challenge, because – to date – it has not been possible to sustain long-term operational stability in perovskite solar cells. Perovskites are ionic materials, and so applying a voltage to a perovskite causes ions to migrate through the material. These migrating ions are believed to contribute to chemical and structural changes in the material that ultimately make it inefficient and unstable. To make practical perovskite solar cells, researchers need to find a way to address this problem.
“We have not found a way to prevent ions from moving through perovskite materials, but we have found that it is possible to steer these ions into a safe conduit that does not impair the material’s structural integrity or performance,” Amassian says. “It’s a big step forward.”
The safe conduit, in this case, is something called a grain boundary. Perovskite materials are multi-crystalline materials. That means that when ‘growing’ a perovskite, the material forms as a series of crystals – or “grains” – that are flush with each other. These grains are responsible for absorbing light and generating the charges responsible for the electrical current. Each of those grains has the same crystalline structure, but they may be oriented in slightly different directions. The area where the grains touch is called a grain boundary.
“What we’ve found is that grains are better protected from impairment when the ions move predominantly along the grain boundary,” says first author and co-corresponding author Masoud Ghasemi, a former postdoctoral researcher at NC State who is now a postdoctoral researcher at Penn State. “Coupling this with what is already known about perovskite materials, it’s clear that problems start when grain boundaries are weak, which makes it easier for ions to move into the grains themselves. Designing stronger grain boundaries that protect the grains is essential to block migrating ions and other harmful species like oxygen from entering the grains, mitigating problematic chemical and structural changes in the material.”
“This is an important insight, because there are established techniques we can use to engineer perovskite materials and their grain boundaries; we can now make use of these approaches to protect the grains,” Amassian says. “We demonstrate how those techniques strengthen grain boundaries in this paper. In short, we now know what needs to be done to make far more stable perovskites.”
This work may also inform the development of more efficient energy-storage technologies. “This work advances our fundamental understanding of how ions move through any crystalline material that can carry charge, not just halide perovskites,” Amassian says. “We’re excited to talk to colleagues who work on energy storage about how this may inform the engineering of faster ion conductors.”
This story is adapted from material from North Carolina State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.