These images show light patterns generated by a rhenium-based crystal using a laser method called optical second-harmonic rotational anisotropy. At left, the pattern comes from the atomic lattice of the crystal. At right, the crystal has become a 3D quantum liquid crystal, showing a drastic departure from the pattern due to the atomic lattice alone. Images: Hsieh Lab/Caltech.Physicists at the Institute for Quantum Information and Matter at the California Institute of Technology (Caltech) have discovered the first three-dimensional (3D) quantum liquid crystal – a new state of matter that may have applications in ultrafast quantum computers of the future.
"We have detected the existence of a fundamentally new state of matter that can be regarded as a quantum analog of a liquid crystal," says Caltech assistant professor of physics David Hsieh, principal investigator on a new paper describing the findings in Science. "There are numerous classes of such quantum liquid crystals that can, in principle, exist; therefore, our finding is likely the tip of an iceberg."
Liquid crystals fall somewhere in between a liquid and a solid: they are made up of molecules that flow around freely as if they were a liquid but are all oriented in the same direction, as in a solid. Liquid crystals can be found in nature, such as in biological cell membranes. Alternatively, they can be made artificially – such as those found in the liquid crystal displays commonly used in watches, smartphones, televisions and other items that have display screens.
In a ‘quantum’ liquid crystal, electrons behave like the molecules in classical liquid crystals. That is, the electrons move around freely yet have a preferred direction of flow. The first-ever quantum liquid crystal was discovered in 1999 by Caltech's Jim Eisenstein, professor of physics and applied physics.
Eisenstein's quantum liquid crystal was two-dimensional (2D), meaning that it was confined to a single plane inside the host material – an artificially-grown gallium-arsenide-based metal. Such 2D quantum liquid crystals have since been found in several more materials including high-temperature superconductors – materials that conduct electricity with zero resistance at around -150°C, which is warmer than the operating temperatures of traditional superconductors.
John Harter, a postdoctoral scholar in the Hsieh lab and lead author of the new study, explains that 2D quantum liquid crystals behave in strange ways. "Electrons living in this flatland collectively decide to flow preferentially along the x-axis rather than the y-axis even though there's nothing to distinguish one direction from the other," he says.
Now Harter and Hsieh, together with colleagues at Oak Ridge National Laboratory and the University of Tennessee have discovered the first 3D quantum liquid crystal. Compared to a 2D quantum liquid crystal, the 3D version is even more bizarre. Here, the electrons not only make a distinction between the x, y and z axes, but they also have different magnetic properties depending on whether they flow forward or backward on a given axis.
"Running an electrical current through these materials transforms them from non-magnets into magnets, which is highly unusual," says Hsieh. "What's more, in every direction that you can flow current, the magnetic strength and magnetic orientation changes. Physicists say that the electrons 'break the symmetry' of the lattice."
Harter actually hit upon this discovery serendipitously. He was originally interested in studying the atomic structure of a metal compound based on the element rhenium. In particular, he was trying to characterize the structure of the crystal's atomic lattice using a technique called optical second-harmonic rotational anisotropy. In these experiments, laser light is fired at a material, and light with twice the frequency is reflected back out. The pattern of emitted light contains information about the symmetry of the crystal. The patterns measured from the rhenium-based metal were very strange – and could not be explained by the known atomic structure of the compound.
"At first, we didn't know what was going on," Harter says. The researchers then learned about the concept of 3D quantum liquid crystals, developed by Liang Fu, a physics professor at MIT. "It explained the patterns perfectly. Everything suddenly made sense," Harter says.
The researchers say that 3D quantum liquid crystals could play a role in a field called spintronics, in which the direction that electrons spin may be exploited to create more efficient computer chips. The discovery could also help with some of the challenges of building a quantum computer, which seeks to take advantage of the quantum nature of particles to produce even faster calculations, such as those needed to decrypt codes.
One of the difficulties in building a quantum computer is that quantum properties are extremely fragile and can easily be destroyed through interactions with their surrounding environment. A technique called topological quantum computing – developed by Alexei Kitaev, professor of theoretical physics and mathematics at Caltech – can solve this problem with the help of a special kind of superconductor dubbed a topological superconductor.
"In the same way that 2D quantum liquid crystals have been proposed to be a precursor to high-temperature superconductors, 3D quantum liquid crystals could be the precursors to the topological superconductors we've been looking for," says Hsieh.
"Rather than rely on serendipity to find topological superconductors, we may now have a route to rationally creating them using 3D quantum liquid crystals" says Harter. "That is next on our agenda."
This story is adapted from material from Caltech, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.