A side view of the diamond anvil cell used to generate pressures above 15 gigapascals between the two synthetic diamonds that are visible near the center of the cell. Photo: Mark Stone/University of Washington.Scientists are excited about diamonds – not the types that adorn jewelry, but the microscopic variety that are less than the width of a human hair. These so-called ‘nanodiamonds’ are made up almost entirely of carbon. But by introducing other elements into the nanodiamond's crystal lattice – a method known as ‘doping’ – researchers could produce traits useful in medical research, computation and beyond.
In a paper in Science Advances, researchers at the University of Washington (UW), the US Naval Research Laboratory and the Pacific Northwest National Laboratory report using extremely high pressures and temperatures to dope nanodiamonds. Using this approach, the team doped nanodiamonds with silicon, causing the diamonds to glow a deep red – a property that would make them useful for cell and tissue imaging.
The team discovered that their method could also be used to dope nanodiamonds with argon, a noble gas and nonreactive element related to the helium found in balloons. Nanodiamonds doped with such elements could be applied to quantum information science – a rapidly expanding field that includes quantum communication and quantum computing.
"Our approach lets us intentionally dope other elements within diamond nanocrystals by carefully selecting the molecular starting materials used during their synthesis," said corresponding author Peter Pauzauskie, a UW associate professor of materials science and engineering and researcher at the Pacific Northwest National Laboratory.
There are other methods for doping nanodiamonds, such as ion implantation, but they often damage the crystal structure and result in the introduced elements being placed randomly, limiting performance and applications. Here, the researchers decided not to dope the nanodiamonds after they had been synthesized. Instead, they doped the molecular ingredients for making nanodiamonds with the element they wanted to introduce, then used high temperatures and pressures to synthesize nanodiamonds with the included elements.
In principle, it's like making a cake: it is far simpler and more effective to add sugar to the batter, rather than trying to add sugar to the cake after baking.
The researchers’ starting point for the nanodiamonds was a carbon-rich material similar to charcoal, which they spun into a lightweight, porous matrix known as an aerogel. They then doped this carbon aerogel with a silicon-containing molecule called tetraethyl orthosilicate, which became chemically integrated within the aerogel. The researchers sealed these reactants within the gasket of a diamond anvil cell, which could generate pressures as high as 15 gigapascals inside the gasket. For reference, 1 gigapascal is roughly 10,000 atmospheres of pressure, or 10 times the pressure at the deepest part of the ocean.
To prevent the aerogel from being crushed at such extreme pressures, the team used argon, which becomes solid at 1.8 gigapascals, as a pressure medium. After loading the material to high pressure, the researchers used a laser to heat the cell above 3100°F, more than one-third the surface temperature of the sun. In collaboration with James Davis, a UW professor emeritus of chemical engineering, the team found that at these temperatures the solid argon melts to form a supercritical fluid.
This process converts the carbon aerogel into nanodiamonds containing luminescent point defects formed from the silicon-based dopant molecules. These defects cause the nanodiamonds to emit a deep-red light at a wavelength of about 740nm, which could be useful in medical imaging. Nanodiamonds doped with other elements could emit other colors.
"We can throw a dart at the periodic table and – so long as the element we hit is soluble in diamond – we could incorporate it deliberately into the nanodiamond using this method," said Pauzauskie. "You could make a wide spectrum of nanodiamonds that emit different colors for imaging purposes. We may also be able to use this molecular doping approach to make more complex point defects with two or more different dopant atoms, including completely new defects that have not been created before."
Unexpectedly, the researchers discovered that their nanodiamonds also contained two other elements that they didn't intend to introduce – the argon used as a pressure medium and nitrogen from the air. Just like the silicon that the researchers had intended to introduce, the nitrogen and argon atoms had been fully incorporated into the nanodiamond's crystal structure.
This marks the first time that scientists have used high-temperature, high-pressure assembly to introduce a noble gas element – argon – into a nanodiamond lattice structure. It is not easy to force nonreactive atoms such as argon to associate with other materials in a compound.
"This was serendipitous, a complete surprise," said Pauzauskie. "But the fact that argon was incorporated into the nanodiamonds means that this method is potentially useful to create other point defects that have potential for use in quantum information science research."
Researchers now plan to dope nanodiamonds intentionally with xenon, another noble gas, for possible use in fields such as quantum communications and quantum sensing.
Finally, the team's method also could help to solve a cosmic mystery. Nanodiamonds have been found in outer space, and something out there – such as supernovae or high-energy collisions – dopes them with noble gases. Though the methods developed by Pauzauskie and his team are for doping nanodiamonds here on Earth, their findings could help scientists learn what types of extraterrestrial events trigger cosmic doping far from home.
This story is adapted from material from the University of Washington, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.