This illustration shows how strontium titanium oxide is combined with graphene strips. The combination opens up a new path to memristive heterostructures combining ferroelectric materials and 2D materials. Image: Banerjee lab, University of Groningen.Scientists are working on new materials to create neuromorphic computers, which have a design based on the human brain. A crucial component is a memristive device, the resistance of which depends on the history of the device – just like the response of our neurons depends on previous input.
Materials scientists from the University of Groningen in the Netherlands have now analyzed the behaviour of strontium titanium oxide, a platform material for memristor research, and used the 2D material graphene to probe it. They report their findings in a paper in ACS Applied Materials and Interfaces.
Computers are giant calculators, full of switches that can have the value of either 0 or 1. Using a great many of these binary systems, computers can perform calculations very rapidly. In other respects, though, computers are not very efficient. Our brain uses less energy for recognizing faces or performing other complex tasks than a standard microprocessor. That is because our brain is made up of neurons that can have many values other than 0 and 1, and because the neurons' output depends on previous input.
To create memristors, switches with a memory of past events, strontium titanium oxide (STO) is often used. This material is a perovskite with a crystal structure that depends on temperature. At low temperatures, it can become an incipient ferroelectric, losing this ferroelectric behaviour at temperatures above 105K. The domains and domain walls that accompany these phase transitions are the subject of active research. Yet, it is still not entirely clear why the material behaves the way it does.
"It is in a league of its own," says Tamalika Banerjee, professor of spintronics of functional materials at the Zernike Institute for Advanced Materials at the University of Groningen.
Oxygen atoms in the crystal appear to be key to its behaviour. "Oxygen vacancies can move through the crystal and these defects are important," explains Banerjee. "Furthermore, domain walls are present in the material and they move when a voltage is applied to it."
Numerous studies have sought to find out how this happens, but looking inside this material is complicated. Banerjee's team has now succeeded in doing this by using another material that is in a league of its own: graphene.
"The properties of graphene are defined by its purity," says Banerjee, "whereas the properties of STO arise from imperfections in the crystal structure. We found that combining them leads to new insights and possibilities."
Much of this work was carried out by Banerjee's PhD student Si Chen. She placed graphene strips on top of a flake of STO and measured the conductivity at different temperatures by sweeping a gate voltage between positive and negative values.
"When there is an excess of either electrons or the positive holes, created by the gate voltage, graphene becomes conductive," Chen explains. "But at the point where there are very small amounts of electrons and holes, the Dirac point, conductivity is limited."
In normal circumstances, the minimum conductivity position does not change with the sweeping direction of the gate voltage. However, in the graphene strips on top of STO, there is a large separation between the minimum conductivity positions for the forward sweep and the backward sweep. The effect is very clear at 4K, but less pronounced at 105K or at 150K. Analysis of the results, along with theoretical studies carried out at Uppsala University, shows that oxygen vacancies near the surface of the STO are responsible.
"The phase transitions below 105K stretch the crystal structure, creating dipoles," says Banerjee. "We show that oxygen vacancies accumulate at the domain walls and that these walls offer the channel for the movement of oxygen vacancies. These channels are responsible for memristive behaviour in STO." Accumulation of oxygen vacancy channels in the crystal structure of STO explains the shift in the position of the minimum conductivity.
Chen also carried out another experiment. "We kept the STO gate voltage at -80V and measured the resistance in the graphene for almost half an hour. In this period, we observed a change in resistance, indicating a shift from hole to electron conductivity." This effect is primarily caused by the accumulation of oxygen vacancies at the STO surface.
Overall, the experiments show that the properties of the combined STO/graphene material change through the movement of both electrons and ions, each at different time scales. "By harvesting one or the other, we can use the different response times to create memristive effects, which can be compared to short-term or long-term memory effects," says Banerjee.
The study creates new insights into the behaviour of STO memristors. "And the combination with graphene opens up a new path to memristive heterostructures combining ferroelectric materials and 2D materials," she adds.
This story is adapted from material from the University of Groningen, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.