Editor in Chief, Eun Kyung Suh, Professor at Chonbuk National University and Executive Editor, Sungkyun Park, from Pusan National University, have recommended the following titles, all of which are free to download:
Structural, morphological, compositional, and optical properties of single step electrodeposited Cu2ZnSnS4 (CZTS) thin films for solar cell application (Volume 14, Issue 3, March 2014, Pages 254–258. Authors: Seul Gi Lee, Jongmin Kim, Huyn Suk Woo, Yongcheol Jo, A.I. Inamdar, S.M. Pawar, Hyung Sang Kim, Woong Jung, Hyun Sik Im)
Oxygen electrocatalysis in chemical energy conversion and storage technologies (Volume 13, Issue 2, March 2013, Pages 309–321. Authors: Jaeyoung Lee, Beomgyun Jeong, Joey D. Ocon)
A new era for liquid crystal research: Applications of liquid crystals in soft matter nano-, bio- and microtechnology (Volume 12, Issue 6, November 2012, Pages 1387–1412. Authors: Jan P.F. Lagerwall, Giusy Scalia)