The mechanical neural network. Photo: Flexible Research Group at UCLA.Mechanical engineers at the University of California, Los Angeles (UCLA) have developed a new class of material that can learn behaviors over time and develop a ‘muscle memory’ of its own, allowing for real-time adaptation to changing external forces.
The material is composed of a structural system made up of tunable beams that can alter their shape and behaviors in response to dynamic conditions. The researchers report the material, which boasts applications in the construction of buildings, airplanes and imaging technologies among others, in a paper in Science Robotics.
“This research introduces and demonstrates an artificial intelligent material that can learn to exhibit the desired behaviors and properties upon increased exposure to ambient conditions,” said Jonathan Hopkins, a mechanical and aerospace engineering professor at the UCLA Samueli School of Engineering, who led the research. “The same foundational principles that are used in machine learning are used to give this material its smart and adaptive properties.”
When the material is placed in aircraft wings, for example, it could learn to morph the shape of the wings based on the wind patterns during a flight to achieve greater efficiency and maneuverability of the plane. Building structures infused with this material could also self-adjust their rigidity in certain areas to improve their overall stability during an earthquake or other natural or man-made disasters.
Utilizing and adapting concepts from existing artificial neural networks (ANNs), which are the algorithms that drive machine learning, the researchers developed the mechanical equivalents of ANN components in an interconnected system. The mechanical neural network (MNN), as the team called it, consists of individually tunable beams oriented in a triangular lattice pattern. Each beam features a voice coil, strain gauges and flexures that allow the beam to change its length, adapt to its changing environment in real time and interact with other beams in the system.
The voice coil, which gets its name from its original use in speakers for converting magnetic fields into mechanical motion, initiates the fine-tuned compression or expansion in response to new forces placed on the beam. The strain gauge is responsible for collecting data from the beam’s motion, while the flexures essentially act as flexible joints among the moveable beams to connect the system.
An optimization algorithm regulates the entire system by taking the data from each of the strain gauges and determining a combination of rigidity values to control how the network should adapt to applied forces. In order to check the validity of the strain gauge-monitored system, the research team also used cameras trained on the output nodes of the system.
Early prototypes of the system exhibited a lag between the input of the applied force and the output of the MNN response, which affected the system’s overall performance. The team tested multiple iterations of the strain gauges and flexures in the beams, as well as different lattice patterns and thicknesses, before achieving their published design, which managed to overcome the lag and accurately distribute the applied force in all directions.
“Identifying the reasons why [the networks] failed to learn is important for understanding how to design MNNs that successfully learn,” the researchers said. They solved this problem through trial and error over the past five years.
Currently, the system is about the size of a microwave oven, but the researchers plan to simplify the MNN design so that thousands of the networks can be manufactured on the micro scale within 3D lattices for practical material applications. Aside from using the material in vehicles and construction materials, the researchers suggest MNNs could also be incorporated into an armor to deflect shockwaves, or in acoustic imaging technologies to harness soundwaves.
This story is adapted from material from UCLA, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.