This image shows 3D-printed crystalline lattice structures with air-filled channels, known as ‘fluidic sensors’, embedded into the structures (the indents on the middle of the lattices are the outlet holes of the sensors). Image courtesy of the researchers, edited by MIT News.Researchers at Massachusetts Institute of Technology (MIT) have developed a method for 3D-printing materials with tunable mechanical properties, which can sense how they are moving and interacting with the environment. The researchers create these sensing structures using just one material and a single run on a 3D printer.
To accomplish this, the researchers begin with 3D-printed lattice materials and incorporate networks of air-filled channels into the structure during the printing process. By measuring how the pressure changes within these channels when the structure is squeezed, bent or stretched, engineers can receive feedback on how the material is moving. The researchers report their work in a paper in Science Advances.
These lattice materials are composed of single cells in a repeating pattern. Changing the size or shape of the cells alters the material’s mechanical properties, such as its stiffness or hardness. For instance, a denser network of cells creates a stiffer structure.
This technique could someday be used to create flexible soft robots with embedded sensors that allow the robots to monitor their posture and movements. It might also be used to produce wearable smart devices, like customized running shoes that provide feedback on how an athlete’s foot is impacting the ground.
“The idea with this work is that we can take any material that can be 3D-printed and have a simple way to route channels throughout it so we can get sensorization with structure. And if you use really complex materials, then you can have motion, perception and structure all in one,” says co-lead author Lillian Chin, a graduate student in the MIT Computer Science and Artificial Intelligence Laboratory (CSAIL).
The researchers focused their efforts on lattices, a type of ‘architected material’, which exhibits customizable mechanical properties based solely on its geometry. For instance, changing the size or shape of the cells in the lattice makes the material more or less flexible.
While architected materials can exhibit unique properties, integrating sensors in them is notoriously challenging. Engineers typically must place sensors on the outside, which is tough because the lattice is full of holes, so there is little material to work with. Also, when sensors are placed on the outside, they are not fully integrated with the material and can be affected by noise that comes from a soft material’s movements.
Instead, Chin and her collaborators used 3D printing to incorporate air-filled channels directly into the struts that form the lattice. When the structure is moved or squeezed, those channels deform and the volume of the air inside changes. The researchers can measure the corresponding change in pressure with an off-the-shelf pressure sensor, which gives feedback on how the material is deforming.
Because they are incorporated into the material, these ‘fluidic sensors’ are more accurate than sensors placed on the outside of a structure.
“If you stretch out a rubber band, it takes a little time to come back into place,” Chin explains. “But since we are using air and the deformations are relatively stable, we don’t get these same time-varying properties. The information that comes out of our sensor is a lot cleaner.”
The researchers incorporate channels into the structure using digital-light-processing 3D printing. In this method, the structure is drawn out of a pool of resin and hardened into a precise shape using projected light. An image is projected onto the wet resin and areas struck by the light are cured.
But as the process continues, the sticky resin tends to drip and get stuck inside the channels. The researchers had to work quickly to remove excess resin before it was cured, using a mix of pressurized air, vacuum and intricate cleaning.
“We will have to do more brainstorming from the design side to think about that cleaning process, since it is the main challenge,” Chin says.
They used this process to create several lattice structures, and demonstrated how the air-filled channels generated clear feedback when the structures were squeezed and bent.
Building off these results, they also incorporated sensors into a new class of materials developed for motorized soft robots known as handed shearing auxetics (HSAs). These materials can be twisted and stretched simultaneously, allowing them to be used as effective soft robotic actuators. But they are difficult to ‘sensorize’ because of their complex forms.
The researchers 3D-printed an HSA soft robot capable of several movements, including bending, twisting and elongating. They ran the robot through a series of movements for more than 18 hours and used the sensor data to train a neural network that could accurately predict the robot’s motion.
Chin was impressed by the results – the fluidic sensors were so accurate she had difficulty distinguishing between the signals the researchers sent to the motors and the data that came back from the sensors.
“Materials scientists have been working hard to optimize architected materials for functionality,” she says. “This seems like a simple, yet really powerful idea to connect what those researchers have been doing with this realm of perception. As soon as we add sensing, then roboticists like me can come in and use this as an active material, not just a passive one.”
“Sensorizing soft robots with continuous skin-like sensors has been an open challenge in the field,” says senior author Daniela Rus, professor of electrical engineering and computer science at MIT and director of CSAIL. “This new method provides accurate proprioceptive capabilities for soft robots and opens the door for exploring the world through touch.”
In the future, Chin looks forward to finding new applications for this technique, such as creating football helmets tailored to a specific player’s head that have sensing capabilities within the internal structure. This could increase the accuracy of feedback from on-field collisions and improve player safety. She is also interested in utilizing machine learning to push the boundaries of tactile sensing for robotics.
This story is adapted from material from MIT, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.