Stefano Curtarolo. Photo: Duke University.A group led by scientists at Duke University has engineered a new class of materials capable of producing tunable plasmonic properties while withstanding incredibly high temperatures.
Plasmonics is a technology that essentially traps the energy of light within groups of electrons oscillating together on a metallic surface. This creates a powerful electromagnetic field that interacts with incoming light, allowing devices to absorb, emit or otherwise control specific frequencies across much of the electromagnetic spectrum.
The new materials are hard enough to stir molten steel and can withstand temperatures above 7000°F – about the same as those found just a few hundred miles above the surface of the Sun. Coupled with their newly discovered plasmonic abilities, these materials could lead to improved communications and thermal regulation in technologies such as satellites and hypersonic aircraft. The scientists report the materials in a paper in Nature Communications.
“The standard metals used in plasmonics research, such as gold, silver and copper, melt at relatively low temperatures and need protection from the elements,” said Arrigo Calzolari, a researcher at the Istituto Nanoscienze of Consiglio Nazionale delle Ricerche in Modena, Italy “That means they can’t be used in rockets, satellites or other aerospace applications. But these new materials we are developing open a completely new working arena because they can create plasmonic effects at incredibly high temperatures.”
The materials come from a class of disordered ceramics called ‘high-entropy’ carbides, discovered in 2018 by Stefano Curtarolo, professor of mechanical engineering and materials science at Duke. Jettisoning the reliance on the crystalline structures and bonds that keep traditional materials together, these high-entropy carbides rely on a combination of many disorderly elements of various sizes to enhance stability. While a pile of baseballs won’t stand on its own, a pile of baseballs, shoes, bats, hats and gloves just might support a resting baseball player.
The original group of high-entropy materials were made of carbon and five different metallic elements, technically making them a class of carbides. Since then, Curtarolo has secured a $7.5 million grant through the US Department of Defense’s Multidisciplinary University Research Initiative (MURI) competition to develop a suite of artificial intelligence tools capable of designing similar materials with tailored properties on demand.
Calzolari knew about these materials and the project Curtarolo was leading. He also knew that tantalum carbide (a parent yet simpler material) is extremely durable and exhibits plasmonic abilities in the visible spectrum. But the material can’t be tuned to different frequencies of light outside its natural range, limiting its usefulness in real-world applications. Putting two and two together, Calzolari and Curtarolo joined forces on a hunch that certain recipes for high-entropy carbides – especially those containing tantalum – could demonstrate tunable plasmonic properties across a wide spectrum.
Less than six months later, they were proven right.
“Arrigo came to me to make sure these carbide mixtures would work and that they would have plasmonic properties,” Curtarolo said. “After running the recipe ideas through the disorder models and calculations we’ve been developing, we discovered that they do have plasmonic properties, and that we can tune them by tweaking the recipes.”
In the paper, the researchers’ models show that 14 different high-entropy recipes demonstrate plasmonic properties across the near-infrared and visible spectrum of light, making them good candidates for optical and telecommunication applications. The researchers also worked with Douglas Wolfe, professor of materials science and engineering at Penn State, to prove their theory experimentally.
As a member of the MURI project led by Curtarolo, Wolfe was already familiar with high-entropy carbides. He happened to have a sample of one of the recipes in question, which helped the group to quickly demonstrate the plasmonic properties of HfTa4C5 and confirm that they matched well with their computational models.
The paper lays out different compositions that work better or worse than each other in various frequency ranges. The researchers plan to continue to create new recipes and test them for potential use in a wide range of applications, including antennas, light and heat manipulation, and many more on any device that is subjected to ultra-high temperatures.
“These materials bring together plasmonics, hardness, stability and high temperatures into a single material,” Curtarolo said. “And they can be tailored to specific applications, which isn’t possible using standard materials because you can’t change properties defined by nature.”
This story is adapted from material from Duke University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.