A magnified image of the new optical waveguide device, featuring a zoomed-in view of the fabricated photonic crystal topological insulator. Image: Natasha Litchinitser, Duke University.Engineers at Duke University have demonstrated a device that can direct photons of light around sharp corners with virtually no losses due to backscattering, a key property that will be needed if electronics are ever to be replaced with light-based devices.
The result was achieved with photonic crystals built on the concept of topological insulators, which won its discoverers a Nobel Prize in 2016. By carefully controlling the geometry of the crystal lattice, the engineers were able to prevent light traveling through the interior of a silicon photonic crystal while transmitting it perfectly along its surface. Using these concepts, the new device accomplishes its near-perfect transmittance around corners despite being much smaller than previous designs.
The Semiconductor Industry Association estimates that the number of electronic devices is increasing so rapidly that by the year 2040, there won't be enough power in the entire world to run them all. One potential solution is to turn to massless photons to replace the electrons currently used for transmitting data. Besides saving energy, photonic systems also promise to be faster and have higher bandwidth.
Photons are already in use in some applications, such as on-chip photonic communication. One drawback of the current technology, however, is that such systems cannot turn or bend light efficiently. But for photons to ever replace electrons in microchips, travelling around corners in microscopic spaces is a necessity.
"The smaller the device the better, but of course we're trying to minimize losses as well," said Wiktor Walasik, a postdoctoral associate in electrical and computer engineering at Duke University. "There are a lot of people working to make an all-optical computing system possible. We're not there yet, but I think that's the direction we're going."
Previous studies have also shown small losses while guiding photons around corners, but the new Duke research does it on a rectangular device just 35µm long and 5.5µm wide – 100 times smaller than previously demonstrated ring-resonator-based devices.
In the new study, which is reported in a paper in Nature Nanotechnology, the engineers fabricated topological insulators using electron beam lithography and measured the light transmittance through a series of sharp turns. The results showed that each turn only resulted in the loss of a few percent of the light.
"Guiding light around sharp corners in conventional photonic crystals was possible before but only through a long laborious process tailored to a specific set of parameters," said Natasha Litchinitser, professor of electrical and computer engineering at Duke University. "And if you made even the tiniest mistake in its fabrication, it lost a lot of the properties you were trying to optimize."
"But our device will work no matter its dimensions or geometry of the photons' path and photon transport is 'topologically protected,'" added Mikhail Shalaev, a doctoral student in Litchinitser's laboratory and first author of the paper. "This means that even if there are minor defects in the photonic crystalline structure, the waveguide still works very well. It is not so sensitive to fabrication errors."
The researchers point out that their device also has a large operating bandwidth, is compatible with modern semiconductor fabrication technologies, and works at wavelengths currently used in telecommunications.
The researchers are next attempting to make their waveguide dynamically tunable to shift the bandwidth of its operation. This would allow the waveguide to be turned on and off at will – another important feature if all-optical photon-based technologies are ever to become a reality.
This story is adapted from material from Duke University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.