Argonne scientists have developed a new polymer coating (shown in blue) for battery cathodes that can improve the electronic and ionic conductivity of a battery while also improving its safety and cycling performance. Image: Argonne National Laboratory.Building a better lithium-ion battery involves addressing a myriad of factors simultaneously, from keeping the battery's cathode electrically and ionically conductive to making sure the battery stays safe after many cycles.
In a new discovery, scientists at the US Department of Energy (DOE)’s Argonne National Laboratory have developed a new cathode coating, using an oxidative chemical vapor deposition technique, that can help solve these and several other potential issues with lithium-ion batteries all in one stroke.
"The coating we've discovered really hits five or six birds with one stone," said Khalil Amine, an Argonne distinguished fellow and battery scientist, who led the research.
As they report in a paper in Nature Energy, Amine and his fellow scientists took particles of Argonne's pioneering nickel-manganese-cobalt (NMC) cathode material and encapsulated them in a sulfur-containing polymer called PEDOT. This polymer provides the cathode with a layer of protection from the battery's electrolyte as the battery charges and discharges.
Unlike conventional coatings, which only protect the exterior surface of the micron-sized cathode particles and leave the interior vulnerable to cracking, the PEDOT coating had the ability to penetrate to the cathode particle's interior, adding an additional layer of shielding.
In addition, although PEDOT prevents the chemical interaction between the battery and the electrolyte, it does allow for the necessary transport of lithium ions and electrons that the battery requires in order to function.
"This coating is essentially friendly to all of the processes and chemistry that makes the battery work, and unfriendly to all of the potential reactions that would cause the battery to degrade or malfunction," said Argonne chemist Guiliang Xu, the first author of the paper.
The coating also largely prevents another reaction that causes the battery's cathode to deactivate. In this reaction, the cathode material transforms into another form called spinel. "The combination of almost no spinel formation with its other properties makes this coating a very exciting material," Amine said.
As an additional benefit, the PEDOT material demonstrated the ability to prevent oxygen release, a major factor in the degradation of NMC cathode materials at high voltage. "This PEDOT coating was also found to be able to suppress oxygen release during charging, which leads to better structural stability and also improves safety," Amine said.
Amine indicated that battery scientists could likely scale up the coating for use in nickel-rich NMC-containing batteries. "This polymer has been around for a while, but we were still surprised to see that it has all of the encouraging effects that it does," he said.
With the coating applied, the scientists believe that NMC-containing batteries could either run at higher voltages – thus increasing their energy output – or have longer lifetimes, or both.
To perform the research, the scientists relied on two DOE Office of Science User Facilities located at Argonne: the Advanced Photon Source (APS) and the Center for Nanoscale Materials (CNM). In situ high-energy X-ray diffraction measurements were taken at beamline 11-ID-C of the APS, and focused ion beam lithography and transmission electron microscopy were performed at the CNM.
This story is adapted from material from Argonne National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.