This image shows how the interplay of multiple mechanisms can be used to form 12 discrete polymer morphologies by modifying the liquid process parameters. Image: Orlin Velev, NC State University.Researchers have developed and demonstrated an efficient and scalable technique that allows them to manufacture soft polymer materials in a dozen different structures, or ‘morphologies’, from ribbons and nanoscale sheets to rods and branched particles. The novel technique allows users to finely tune the morphology of the materials at the micro- and nanoscale.
“This advance is important because the technique can be used with a wide variety of polymers and biopolymers,” says Orlin Velev, distinguished professor of chemical and biomolecular engineering at North Carolina State University (NC State) and corresponding author of a paper on this work in Advanced Materials. “Since the morphology of these polymeric micro- and nanostructures is critical for their applications, it allows us to obtain new polymer functionalities by simply controlling structure instead of polymer chemistry. For example, the nanosheets can be used in designing better batteries, whereas dendricolloids – branching networks of polymer fibers that have exceptionally high surface area – can be used in environmental remediation technologies or creation of novel lightweight metamaterials.”
Fundamentally, all of the different morphologies are produced using a well-known process called polymer precipitation. In this process, a polymer is dissolved into a solvent, producing a polymer solution. That polymer solution is then introduced into a second liquid, which makes the polymer come back together as soft matter.
What’s new in this case is that the researchers have discovered how to precisely control the structure of the resulting polymer soft matter by manipulating three sets of parameters during the manufacturing process.
The first set of parameters is the shear rate, which refers to how quickly the liquids are stirred when they are mixed together. The second set of parameters is the concentration of the polymer in the polymer solution. The last set of parameters is the composition of the solvent that the polymer was initially dissolved in, as well as the composition of the liquid that the polymer solution is added to.
“We identified the critical parameters that affect the final morphology of the polymeric materials, which in turn gives us a great deal of control and versatility” says Rachel Bang, first author of the paper and a recent PhD graduate from NC State. “Because we now understand the role of each of these factors and how they all influence each other, we can reproducibly fine-tune the polymeric particle morphology.”
“Even though we have demonstrated how to produce a dozen different morphologies, we are still in the early stages of exploring all of the possible outcomes and applications,” Velev adds.
The researchers have already demonstrated that the dendricolloids can be used to make membranes for growing live cells, or to create hydrophobic and hydrophilic coatings. They have also worked with collaborators to demonstrate that the nanosheets show potential for use as more efficient separators in lithium-ion batteries.
“The technique can also be used with a variety of natural biopolymers, such as plant proteins, and it could be used to support a variety of applications, such as the development of plant-based meat analogues, which requires precise control of protein particle morphologies at multiple length scales,” says co-author Simeon Stoyanov of the Singapore Institute of Technology and Wageningen University in the Netherlands. “In addition, because our technique is based on mixing liquids using conventional mixers, it can be easily scaled up for practical manufacturing.”
“We are currently working with food science researchers to determine how protein microrods could be used to control the texture of some food products,” Velev says. “And we are also working with collaborators to explore how our technique can be used to produce biopolymer-based materials for use in biodegradable soft electronics.
“We are open to working with additional collaborators to explore potential applications for the polymers and biopolymers across all of these morphologies.”
This story is adapted from material from North Carolina State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.