Researchers have developed a new mechanism to make water droplets slip off surfaces. This discovery, reported in a paper in Nature Chemistry, challenges existing ideas about friction between solid surfaces and water and opens up a new avenue for studying droplet slipperiness at the molecular level. The new technique has applications in a range of fields, including plumbing, optics, and the auto and maritime industries.
All around us, water is always interacting with solid surfaces. Cooking, transportation, optics and hundreds of other technologies are affected by how water sticks to surfaces or slides off them. Understanding the molecular dynamics of these microscopic droplets helps scientists and engineers find ways to improve many household and industrial technologies.
Liquid-like surfaces are a new type of droplet-repellent surface that offer many technical benefits over traditional approaches and were recently reviewed in a paper in Nature Reviews Chemistry by Robin Ras, a professor at Aalto University in Finland. They have molecular layers that are highly mobile yet covalently tethered to a substrate, giving solid surfaces a liquid-like quality that resembles a layer of lubricant between the water droplets and the surface itself.
In this study, a research team led by Ras used a specially designed reactor to create a liquid-like layer of molecules, called a self-assembled monolayer (SAM), on top of a silicon surface.
“Our work is the first time that anyone has gone directly to the nanometer-level to create molecularly heterogenous surfaces,” says Sakari Lepikko, a doctoral researcher at Aalto University and lead author of the paper.
By carefully adjusting conditions such as temperature and water content inside the reactor, the team could fine-tune how much of the silicon surface the monolayer covered.
“I find it very exciting that by integrating the reactor with an ellipsometer, that we can watch the self-assembled monolayers grow with extraordinary level of detail,” says Ras.
“The results showed more slipperiness when SAM coverage was low or high, which are also the situations when the surface is most homogeneous. At low coverage, the silicon surface is the most prevalent component, and at high, SAMs are the most prevalent.”
“It was counterintuitive that even low coverage yielded exceptional slipperiness,” Lepikko adds.
At low coverage, the water forms a film over the surface, which had been thought to increase the amount of friction. “We found that, instead, water flows freely between the molecules of the SAM at low SAM coverage, sliding off the surface. And when the SAM coverage is high, the water stays on top of the SAM and slides off just as easily. It’s only in between these two states that water adheres to the SAMs and sticks to the surface.”
The new method proved exceptionally effective, as the team created the slipperiest liquid surface in the world.
This discovery promises to have implications wherever droplet-repellent surfaces are needed. According to Lepikko, this covers hundreds of examples, from daily life to industrial solutions.
“Things like heat transfer in pipes, de-icing and anti-fogging are potential uses,” Lepikko says. “It will also help with microfluidics, where tiny droplets need to be moved around smoothly, and with creating self-cleaning surfaces. Our counterintuitive mechanism is a new way to increase droplet mobility anywhere it’s needed.”
Next, the team plans to continue experimenting with their SAM setup and improve the layer itself. Lepikko is particularly excited about the information this work has provided for future innovations.
“The main issue with a SAM coating is that it’s very thin, and so it disperses easily after physical contact. But studying them gives us fundamental scientific knowledge which we can use to create durable practical applications.”
This story is adapted from material from Aalto University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.