This photo shows Fang Ren, who developed algorithms to analyze data on the fly while a postdoctoral scholar at SLAC, at a Stanford Synchrotron Radiation Lightsource beamline. Photo: Dawn Harmer/SLAC National Accelerator Laboratory.Blend two or three metals together and you get an alloy that usually looks and acts like a metal, with its atoms arranged in rigid geometric patterns.
But once in a while, under just the right conditions, you get something entirely new: a futuristic alloy called metallic glass that's amorphous, with its atoms arranged every which way, much like the atoms of the glass in a window. Its glassy nature makes it stronger and lighter than today's best steel, plus it stands up better to corrosion and wear.
Even though metallic glass shows a lot of promise as a protective coating and alternative to steel, only a few thousand of the millions of possible combinations of ingredients have been evaluated over the past 50 years, and only a handful developed to the point that they may become useful.
Now, a group led by scientists at the US Department of Energy (DOE)'s SLAC National Accelerator Laboratory, the US National Institute of Standards and Technology (NIST) and Northwestern University has reported a shortcut for discovering and improving metallic glass – and, by extension, other elusive materials – at a fraction of the time and cost.
The research group took advantage of a system at SLAC's Stanford Synchrotron Radiation Lightsource (SSRL) that combines machine learning – a form of artificial intelligence (AI) where computer algorithms glean knowledge from enormous amounts of data – with experiments that quickly make and screen hundreds of sample materials at a time. As the group reports in a paper in Science Advances, this allowed them to discover three new blends of ingredients that form metallic glass, and to do it 200 times faster than could be done before.
"It typically takes a decade or two to get a material from discovery to commercial use," said Chris Wolverton, a professor at Northwestern and early pioneer in using computation and AI to predict new materials, who was a co-author of the paper. "This is a big step in trying to squeeze that time down. You could start out with nothing more than a list of properties you want in a material and, using AI, quickly narrow the huge field of potential materials to a few good candidates."
The ultimate goal, he said, is to get to the point where a scientist could scan hundreds of sample materials, get almost immediate feedback from machine learning models and have another set of samples ready to test the next day – or even within the hour.
Over the past half century, scientists have investigated about 6000 combinations of ingredients that form metallic glass, said paper co-author Apurva Mehta, a staff scientist at SSRL. "We were able to make and screen 20,000 in a single year."
Other groups have used machine learning to come up with predictions about where different kinds of metallic glass can be found. "The unique thing we have done is to rapidly verify our predictions with experimental measurements and then repeatedly cycle the results back into the next round of machine learning and experiments," Mehta said.
There's plenty of room to make the process even speedier, he added, and eventually automate it to take people out of the loop altogether, so scientists can concentrate on other aspects of their work that require human intuition and creativity. "This will have an impact not just on synchrotron users, but on the whole materials science and chemistry community," Mehta said.
According to the team, this method will be useful in all kinds of experiments, especially conducting searches for materials like metallic glass and catalysts whose performance is strongly influenced by the way they're manufactured, and those where scientists don't have theories to guide their search. With machine learning, no previous understanding is needed. The algorithms make connections and draw conclusions on their own, and this can steer research in unexpected directions.
"One of the more exciting aspects of this is that we can make predictions so quickly and turn experiments around so rapidly that we can afford to investigate materials that don't follow our normal rules of thumb about whether a material will form a glass or not," said paper co-author Jason Hattrick-Simpers, a materials research engineer at NIST. "AI is going to shift the landscape of how materials science is done, and this is the first step."
This paper is the first scientific result associated with a DOE-funded pilot project in which SLAC is working with a Silicon Valley AI company called Citrine Informatics to transform the way new materials are discovered and make the tools for doing that available to scientists everywhere.
Founded by former graduate students from Stanford and Northwestern universities, Citrine has created a materials science data platform where data that had been locked away in published papers, spreadsheets and lab notebooks is stored in a consistent format. This allows it to be analyzed using AI specifically designed for materials.
"We want to take materials and chemical data and use them effectively to design new materials and optimize manufacturing," said Greg Mulholland, founder and CEO of the company. "This is the power of artificial intelligence: as scientists generate more data, it learns alongside them, bringing hidden trends to the surface and allowing scientists to identify high-performance materials much faster and more effectively than relying on traditional, purely human-driven materials development."
Until recently, thinking up, making and assessing new materials was painfully slow. The authors of the metallic glass paper calculated that even if you could cook up and examine five potential types of metallic glass a day, every day of the year, it would take more than a thousand years to plow through every possible combination of metals. And when they do discover a metallic glass, researchers often struggle to overcome problems that can hold these materials back. Some have toxic or expensive ingredients, and all of them share glass's brittle, shatter-prone nature.
Over the past decade, scientists at SSRL and elsewhere have developed ways to automate experiments so they can create and study more novel materials in less time. Today, some SSRL users can get a preliminary analysis of their data almost as soon as it comes out using AI software developed by SSRL in conjunction with Citrine and the CAMERA project at DOE's Lawrence Berkeley National Laboratory.
"With these automated systems we can analyze more than 2000 samples per day," said Fang Ren, the paper's lead author, who developed algorithms to analyze data on the fly and coordinated their integration into the system while a postdoctoral scholar at SLAC.
In the metallic glass study, the research team investigated thousands of alloys that each contain three cheap, nontoxic metals. They started with a trove of materials data dating back more than 50 years, including the results of 6000 experiments that searched for metallic glass. The team combed through the data with advanced machine learning algorithms developed by Wolverton and graduate student Logan Ward at Northwestern.
Based on what the algorithms learned in this first round, the scientists crafted two sets of sample alloys using two different methods, allowing them to test how manufacturing methods affect whether an alloy morphs into a glass.
Both sets of alloys were scanned by an SSRL X-ray beam and the resultant data fed into the Citrine database to generate new machine learning results. These were then used to prepare new samples that underwent another round of scanning and machine learning.
By the experiment's third and final round, Mehta said, the group's success rate for finding metallic glass had increased from one out of 300 or 400 samples tested to one out of two or three samples tested. The metallic glass samples they identified represented three different combinations of ingredients, two of which had never been used to make metallic glass before.
This story is adapted from material from SLAC National Accelerator Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.