This Illustration shows the molecular structure of the graphene nanoribbons. Image courtesy of Yves Rubin.Silicon – the shiny, brittle metal commonly used to make semiconductors – is an essential ingredient of modern-day electronics. But as electronic devices have become smaller and smaller, creating tiny silicon components that fit inside them has become more challenging and expensive.
Now, chemists at the University of California, Los Angeles (UCLA) have developed a new method to produce nanoribbons of graphene, next-generation structures that many scientists believe will one day power electronic devices. They describe this new method in a paper in the Journal of the American Chemical Society.
The nanoribbons are extremely narrow strips of graphene, the width of just a few carbon atoms. They're useful because, unlike normal graphene, they possess a bandgap, which means that electrons must be ‘pushed’ to flow through them to create electrical current.
"A material that has no bandgap lets electrons flow through unhindered and cannot be used to build logic circuits," said Yves Rubin, a professor of chemistry at UCLA and lead author of the research.
Rubin and his research team constructed graphene nanoribbons molecule-by-molecule using a simple reaction based on ultraviolet light and exposure to temperatures of 600°C.
"Nobody else has been able to do that, but it will be important if one wants to build these molecules on an industrial scale," said Rubin, who also is a member of the California NanoSystems Institute at UCLA.
The process improves upon other existing methods for creating graphene nanoribbons, one of which involves snipping open tubes of graphene known as carbon nanotubes. That particular approach is imprecise and produces ribbons of inconsistent widths, which is a problem because the size of a nanoribbon's bandgap depends on its width, Rubin said.
To create the nanoribbons, the scientists started by growing crystals of four different colorless molecules. The crystals locked the molecules into the perfect orientation to react, and the team then used light to stitch the molecules into polymers.
The scientists placed the shiny, deep blue polymers in an oven containing only argon gas and heated them to 600°C. The heat provided the necessary boost of energy for the polymers to form the final bonds that gave the nanoribbons their final shape: hexagonal rings composed of carbon atoms, with hydrogen atoms along the edges of the ribbons.
"We're essentially charring the polymers, but we're doing it in a controlled way," Rubin said.
The process, which took about an hour, yielded graphene nanoribbons just eight carbon atoms wide but thousands of atoms long. The scientists verified the molecular structure of the nanoribbons, which were deep black in color and lustrous, by shining light of different wavelengths at them.
"We looked at what wavelengths of light were absorbed," Rubin said. "This reveals signatures of the structure and composition of the ribbons."
The researchers have filed a patent application for the process. Rubin said the team is now studying how to better manipulate the nanoribbons – a challenge because they tend to stick together.
"Right now, they are bundles of fibers," Rubin said. "The next step will be able to handle each nanoribbon one by one."
This story is adapted from material from UCLA, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.