Shown here are the three gas regimes in MOFs: (A) gas adsorbates interact with pore walls (green arrows); (B) gas adsorbates interact with each other within a pore (blue arrows); (C) gas molecules interact with each other across pore walls (red arrows). Light blue molecules are adsorbed onto the internal pore surface; yellow molecules are adsorbed in the center of the pores. Image: Berkeley Lab.An international team of scientists has developed a technique termed ‘gas adsorption crystallography’ that provides a new way to study the process by which metal-organic frameworks (MOFs) store immense volumes of gases such a carbon dioxide, hydrogen and methane. This new look at MOFs – 3D crystals with extraordinarily large internal surface areas – led to a discovery that holds promise for the improved design of MOFs tailored specifically for capturing carbon capture, or storing hydrogen and natural gas (methane) fuels.
"Up to this point we have been shooting in the dark in our designing of MOFs without really understanding the fundamental reasons for why one MOF is better than another," says team leader Omar Yaghi, a renowned chemist with the Lawrence Berkeley National Laboratory (Berkeley Lab). "Our new study expands our view and thinking about MOFs by introducing gas-gas interactions and their organization into superlattices that are a major factor in achieving high storage capacity for gases."
Yaghi, who invented MOFs in the early 1990s while at the Arizona State University, is now a faculty scientist with Berkeley Lab's Materials Sciences Division and the University of California (UC) Berkeley’s Chemistry Department, where he also serves as co-director of the Kavli Energy NanoScience Institute. For this latest study, Yaghi and Osamu Terasaki, a chemist at Stockholm University, along with collaborators from institutes in the US, China, South Korea and Saudi Arabia, interfaced a gas adsorption apparatus with a form of X-ray crystallography called in-situ small angle X-ray scattering (SAXS). The result was a gas adsorption crystallography technique that uncovered evidence of cooperative interactions between gas molecules within a MOF.
"These cooperative gas-gas interactions lead to highly organized behavior, which results in the formation of gas aggregates about 40nm in size," Yaghi says. "The aggregates are arranged in orderly superlattice structures, which is in stark contrast to the prevailing view that the adsorption of gas molecules by MOFs occurs stochastically." Yaghi and Terasaki are the corresponding authors of a paper describing this study that has been published in Nature.
Since Yaghi's original invention, thousands of different types of MOFs have been created. A typical MOF consists of a metal oxide center surrounded by organic molecules that form a highly porous three-dimensional crystal framework. The variations on this basic structure are virtually limitless, allowing the synthesis of MOFs with pores that adsorb specific gas molecules, making MOFs potentially ideal gas storage vessels.
"One gram of MOF has a surface area of up to 10,000m2 onto which it is possible to compact gas molecules into MOF pores like so many bees on a honeycomb without the high pressures and low temperatures usually required for compressed gas storage," Yaghi says.
The selectivity and uptake capacity of a MOF are determined by the nature of the gas molecule being adsorbed and its interactions with the MOF's constituent molecules. While the interactions of gas molecules with the internal surface of a MOF and among themselves within individual pores have been extensively studied, the gas-gas interactions across a MOF's pore walls have not been explored until now.
With their SAXS-based gas adsorption crystallography technique, Yaghi, Terasaki and their collaborators discovered that local strain in the MOF induced by pore-filling can give rise to collective and long-range gas-gas interactions, resulting in the formation of superlattices that extend over several pores.
"We were able to track and map the distribution and ordering of adsorbate molecules in five members of the mesoporous MOF-74 series along entire adsorption-desorption isotherms," Yaghi says. "In all cases, we found that the capillary condensation that fills the pores gives rise to the formation of extra-adsorption domains that span several neighboring pores and have a higher adsorbate density than non-domain pores."
The next step, Yaghi says, will be to apply this new gas adsorption crystallography technique to other porous molecular systems that can serve as gas storage vessels, such as covalent organic frameworks (COFs) and zeolitic imidazolate frameworks (ZIFs).
"We want to generate a comprehensive view of how various gases interact collectively within porous materials interior," says Yaghi. "We will then feed this data into computer models to improve the theory of gas adsorption."
This story is adapted from material from the Lawrence Berkeley National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.