Radiative-cooling devices offer electricity-free cooling by radiating heat at wavelengths that are not absorbed by the Earth’s atmosphere and so escape to outer space. Image: 2023 KAUST; Xavier Pita.In a world experiencing increased heat stress, a zero-carbon-emission cooling technology that consumes no electricity, operating instead by shedding heat directly into outer space, would be a groundbreaking advance. However, poor standardization and a lack of transparency is hampering this promising technology, known as radiative cooling.
Now, in a paper in Nature Sustainability, a team led by Qiaoqiang Gan, a leading radiative-cooling researcher at King Abdullah University of Science & Technology (KAUST) in Saudi Arabia, has outlined best-practice guidelines that could help set the research field back on track.
Radiative-cooling devices offer electricity-free cooling by radiating heat within a narrow wavelength range called the atmospheric transparent window. Within this window, heat is not reabsorbed by the atmosphere and instead escapes into space, which, at three degrees above absolute zero, acts as a vast heat sink and readily soaks up the emitted heat.
“The technology is particularly attractive to address local cooling needs in Saudi Arabia,” Gan says.
Many materials display radiative cooling at night. “The key challenge is to achieve cooling to below ambient temperatures while under direct sunlight,” Gan says. “One must simultaneously minimize the heating effect of solar absorption while maximizing thermal emission in the atmospheric window.” Despite the challenge, there is rapidly growing interest in this sustainable cooling technology due to its potential to counter the impact of global warming.
However, there are numerous potential pitfalls when testing and reporting new radiative-cooling materials. As radiative cooling uses the sky as a heat sink, most experiments are conducted in the local outdoor environment.
“Due to uncontrollable weather conditions and variations in measurement settings, it becomes challenging to compare and comprehend the actual cooling performance of different technologies, and so to identify the best strategies among the various radiative cooling designs being studied,” Gan says.
“After discussing these issues with a senior editor at Nature Sustainability, we were invited to write an article proposing standardized criteria and characterization procedures for evaluating radiative cooling performance.”
His team developed clear recommendations for radiative-cooling material characterization – and procedures for calculating cooling – to improve the reliability and comparability of radiative-cooling research.
“We hope this framework will contribute to the advancement of sustainable and efficient cooling solutions,” Gan says. Considering the extreme heatwave experienced in 2022 and the record-breaking high temperatures observed in numerous major cities during the first half of 2023, the need for electricity-free cooling solutions has become more critical than ever.
“By leveraging radiative cooling, which has the potential for zero or even negative carbon emissions, we can effectively address this global challenge and support the Saudi national strategic plan of Vision 2030.”
This story is adapted from material from KAUST, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.