Data from the team’s neutron scattering experiments showed strong correlations between KYbSe2 and the simulated spectrum of a quantum spin liquid state. Image: Allen Scheie/Los Alamos National Laboratory, U.S. Dept. of Energy.In 1973, physicist Phil Anderson hypothesized that the quantum spin liquid (QSL) state existed in some triangular atomic lattices, but he lacked the tools to delve deeper. Fifty years later, a team led by researchers associated with the Quantum Science Center (QSC), headquartered at the US Department of Energy (DOE)’s Oak Ridge National Laboratory (ORNL), has confirmed the presence of QSL behavior in a new material with a triangular structure – KYbSe2. The researchers report their findings in a paper in Nature Physics.
QSLs – an unusual state of matter controlled by interactions among entangled, or intrinsically linked, magnetic atoms called spins – excel at stabilizing quantum mechanical activity in KYbSe2 and other delafossites. These materials are prized for their layered triangular lattices and promising properties that could contribute to the construction of high-quality superconductors and quantum computing components.
“Researchers have studied the triangular lattice of various materials in search of QSL behavior,” said Allen Scheie, a staff scientist at Los Alamos National Laboratory, QSC member and lead author of the paper. “One advantage of this one is that we can swap out atoms easily to modify the material’s properties without altering its structure, and this makes it pretty ideal from a scientific perspective.”
Using a combination of theoretical, experimental and computational techniques, the team observed multiple hallmarks of QSLs in KYbSe2: quantum entanglement, exotic quasiparticles and the right balance of exchange interactions, which control how a spin influences its neighbors. Although efforts to identify these features have historically been hindered by the limitations of physical experiments, modern neutron scattering instruments can produce accurate measurements of complex materials at the atomic level.
By examining KYbSe2’s spin dynamics with the Cold Neutron Chopper Spectrometer at ORNL’s Spallation Neutron Source (SNS) – a DOE Office of Science user facility – and comparing the results to trusted theoretical models, the researchers found evidence that the material was close to the quantum critical point at which QSL characteristics thrive. They then analyzed its single-ion magnetic state with SNS’s Wide-Angular-Range Chopper Spectrometer.
The evidence comes in the form of one-tangle, two-tangle and quantum Fisher information, which played a key role in previous QSC research examining a 1D spin chain, or a single line of spins within a material. KYbSe2 is a 2D system, a quality that made these endeavors more complex.
“We are taking a co-design approach, which is hardwired into the QSC,” said Alan Tennant, a professor of physics and materials science and engineering at the University of Tennessee, Knoxville, who leads a quantum magnets project for the QSC. “Theorists within the center are calculating things they haven’t been able to calculate before, and this overlap between theory and experiment enabled this breakthrough in QSL research.”
This study aligns with the QSC’s priorities, which include connecting fundamental research to quantum electronics, quantum magnets and other current and future quantum devices.
“Gaining a better understanding of QSLs is really significant for the development of next-generation technologies,” Tennant said. “This field is still in the fundamental research state, but we can now identify which materials we can modify to potentially make small-scale devices from scratch.”
Although KYbSe2 is not a true QSL, the fact that about 85% of its magnetism fluctuates at low temperature means that it has the potential to become one. The researchers anticipate that slight alternations to its structure or exposure to external pressure could potentially help it reach 100%.
QSC experimentalists and computational scientists are planning parallel studies and simulations focused on delafossite materials, but the researchers’ findings establish an unprecedented protocol that can also be applied to the study of other systems. By streamlining evidence-based evaluations of QSL candidates, they aim to accelerate the search for genuine QSLs.
“The important thing about this material is that we’ve found a way to orient ourselves on the map so to speak and show what we’ve gotten right,” Scheie said. “We’re pretty sure there’s a full QSL somewhere within this chemical space, and now we know how to find it.”
This story is adapted from material from Oak Ridge National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.