UCLA researchers have discovered that, in the absence of corrosion, lithium forms a 12-sided figure known as a rhombic dodecahedron on electrode surfaces. Image: Li Lab/UCLA.Rechargeable lithium-ion batteries power smartphones, electric vehicles, and storage for solar and wind energy, among other technologies. But a related battery technology, the lithium-metal battery, hasn’t been developed or adopted as broadly. The reason for this is that while lithium-metal batteries have the potential to hold around double the energy of lithium-ion batteries, they present a far greater risk of catching fire or even exploding.
Now, members of the California NanoSystems Institute at the University of California, Los Angeles (UCLA) have made a fundamental discovery that could lead to safer lithium-metal batteries that outperform today’s lithium-ion batteries. They report their work in a paper in Nature.
Metallic lithium reacts so easily with chemicals that, under normal conditions, corrosion forms almost immediately when the metal is being laid down on a surface such as an electrode. But the UCLA investigators developed a technique to prevent this corrosion and showed that, in its absence, lithium atoms assemble into a surprising shape – the rhombic dodecahedron, a 12-sided figure similar to the dice used in role-playing games like Dungeons and Dragons.
“There are thousands of papers on lithium metal, and most descriptions of the structure is qualitative, such as ‘chunky’ or ‘column-like’,” said Yuzhang Li, an assistant professor of chemical and biomolecular engineering at the UCLA Samueli School of Engineering, a member of CNSI and corresponding author of the paper. “It was surprising for us to discover that when we prevented surface corrosion, instead of these ill-defined shapes, we saw a singular polyhedron that matches theoretical predictions based on the metal’s crystal structure. Ultimately, this study allows us to revise how we understand lithium-metal batteries.”
At tiny scales, a lithium-ion battery stores positively charged lithium atoms in a cage-like structure of carbon that coats an electrode. By contrast, a lithium-metal battery uses an electrode coated with metallic lithium. This electrode packs 10 times more lithium into the same space, compared with a carbon-coated electrode, which accounts for the increase in both performance and danger.
The process for laying down the lithium coating is based on a 200-plus-year-old technique that employs electricity and solutions of salts called electrolytes. Often, the lithium forms microscopic branching filaments with protruding spikes. In a battery, if two of those spikes crisscross, it can cause a short circuit that could lead to an explosion.
The revelation of the true shape of lithium – that is, in the absence of corrosion – suggests that the explosion risk for lithium-metal batteries can be abated, because without corrosion the atoms accumulate in an orderly form instead of one that can crisscross. This discovery could also have substantial implications for high-performance energy technology.
“Scientists and engineers have produced over two decades’ worth of research into synthesizing metals including gold, platinum and silver into shapes such as nanocubes, nanospheres and nanorods,” Li said. “Now that we know the shape of lithium, the question is can we tune it so that it forms cubes, which can be packed in densely to increase both the safety and performance of batteries?”
Until now, the prevailing view had been that the choice of electrolytes in solution determines the shape that lithium forms on a surface – whether the structure resembles chunks or columns. The UCLA researchers had a different idea.
“We wanted to see if we could deposit lithium so quickly that we outpace the reaction that causes the corrosion film,” said UCLA doctoral student Xintong Yuan, the paper’s first author. “That way, we could potentially see how the lithium wants to grow in the absence of that film.”
The researchers developed a new technique for depositing lithium faster than the corrosion forms. They ran current through a much smaller electrode in order to push electricity out faster – much like the way that partially blocking the nozzle of a garden hose causes water to shoot out more forcefully.
A balance was required, however, because speeding up the process too much would lead to the same spiky structures that cause short circuits. The team addressed that issue by adjusting the shape of their tiny electrode.
They laid down lithium on surfaces using four different electrolytes, comparing the results with a standard technique to their new method. With corrosion, the lithium formed four distinct microscopic shapes. With their corrosion-free process, however, they found that the lithium formed miniscule dodecahedrons – no bigger than 2µm– in all four cases.
The researchers were able to see the shape of lithium thanks to an imaging technique called cryo-electron microscopy (cryo-EM), which beams electrons through frozen samples to show details down to the atomic level while inhibiting damage to the samples. Cryo-EM has become ubiquitous in biosciences for determining the structures of proteins and viruses. Its use for materials science is growing, and the UCLA researchers had two key advantages.
First, when Li was a graduate student, he demonstrated that cryo-EM can be used to analyze lithium, which falls to pieces when exposed to an electron beam at room temperature. Second, the team performed experiments at CNSI’s Electron Imaging Center for Nanomachines, which is home to several cryo-EM instruments that have been customized to accommodate the types of samples used in materials research.
This story is adapted from material from UCLA, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.