Solar panels: Photo: OSU.A team of scientists led by a researcher at Oregon State University (OSU) has developed a new electrolyte that raises the efficiency of the zinc-metal anode in zinc batteries to nearly 100%. This represents a breakthrough in the development of an alternative to lithium-ion batteries for large-scale energy storage.
The research is part of an ongoing global quest for new battery chemistries able to store renewable solar and wind energy for use when the Sun isn’t shining and the wind isn’t blowing. Xiulei ‘David’ Ji of the OSU College of Science and colleagues, including from HP Inc. and GROTTHUSS INC., an Oregon State spinout company, report this work in a paper in Nature Sustainability.
“The breakthrough represents a significant advancement toward making zinc-metal batteries more accessible to consumers,” Ji said. “These batteries are essential for the installation of additional solar and wind farms. In addition, they offer a secure and efficient solution for home energy storage, as well as energy-storage modules for communities that are vulnerable to natural disasters.”
A battery stores electricity in the form of chemical energy, and through reactions converts this to electrical energy. There are many different types of batteries, but most of them work in the same basic way and contain the same basic components.
Every battery has two electrodes – the anode, from which electrons flow out into an external circuit, and the cathode, which receives electrons from the external circuit – and an electrolyte, the chemical medium that separates the electrodes and allows the flow of ions between them.
Relying on a metal that’s safe and abundant, zinc-based batteries are energy dense and seen as a possible alternative to widely used lithium-ion batteries for grid energy storage, The production of lithium-ion batteries also relies on shrinking supplies of rare metals such as cobalt and nickel, which are toxic and can contaminate ecosystems and water sources if they leach out of landfills.
Additionally, the electrolytes in lithium-ion batteries are commonly dissolved in flammable organic solvents that often decompose at high operation voltages. Other safety concerns include dendrites, which resemble tiny trees growing inside a battery. These dendrites can pierce the separator between the two electrodes, like thistles growing through cracks in a driveway, leading to unwanted and sometimes unsafe chemical reactions.
“Zinc-metal batteries are one of the leading candidate technologies for large-scale energy storage,” Ji said. “Our new hybrid electrolyte uses water and an ordinary battery solvent, which is non-flammable, cost-effective and of low environmental impact. The electrolyte is made of a dissolved mixture of inexpensive chloride salts, with the primary one being zinc chloride.”
The cost of electricity delivered by a storage facility consisting of zinc batteries can only be competitive with fossil-fuel-produced electricity if the battery can continue operating for thousands of cycles, Ji said. To date, however, the cycle life of zinc batteries has been limited by the poor reversibility performance of the zinc anode.
During charging, zinc cations in the electrolyte gain electrons and get plated on the surface of the anode. During discharge, the plated anode gives up its electrons as the zinc cations are dissolved back into the electrolyte.
“This zinc plating and dissolution process is often woefully irreversible,” Ji said. “Namely, some electrons used in plating cannot be recouped during discharge. This is a problem in an area known as Coulombic efficiency.”
Coulombic efficiency (CE) is a measure of how well electrons are transferred in batteries; specifically, it is the ratio of the total charge extracted from the battery to the charge put in the over a full cycle. Lithium-ion batteries can have a CE in excess of 99%.
The new electrolyte developed by Ji and his collaborators, which included scientists at the Massachusetts Institute of Technology, Penn State and the University of California (UC) Riverside, gave rise to a CE of 99.95%.
“The primary challenge with zinc batteries is that zinc reacts with water in the electrolyte to generate hydrogen gas in what is called a hydrogen-evolution reaction,” Ji said. “This parasitic reaction causes a short cycle life and is also a potential safety hazard.”
The new electrolyte restricts water’s reactivity and nearly shuts down the hydrogen-evolution reaction by forming a ‘passivation layer’ on the surface of the anode. A similar passivation layer is what enabled the initial commercialization of lithium-ion batteries in the 1990s.
Ji credits OSU chemistry colleague Chong Fang for uncovering the electrolyte’s atomic structure using femtosecond Raman spectroscopy and Alex Greaney at UC Riverside for determining the passivation mechanism.
“Also, it is worth noting that the efficiency we measured is under harsh conditions that do not mask any damage caused by the hydrogen-evolution reaction,” Ji added. “The breakthrough reported here heralds the near-future commercialization of the zinc-metal batteries for large-scale grid storage.”
This story is adapted from material from Oregon State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.