Electrons from a heated light filament (top) land on solid neon (red block), where a single electron (represented as a wave function in blue) is trapped and manipulated by a superconducting quantum circuit (bottom patterned chip). Image: Dafei Jin/Argonne National Laboratory.In today’s digital devices, the basic unit of information is the bit, which can be either 0 or 1. But scientists worldwide are now racing to develop a new kind of computer based on the use of quantum bits, or qubits.
In a paper in Nature, a team led by researchers at the US Department of Energy (DOE)’s Argonne National Laboratory report the creation of a new qubit platform formed by freezing neon gas into a solid at very low temperatures, spraying electrons from a light bulb’s filament onto this solid and trapping a single electron there. This system shows great promise to be developed into ideal building blocks for future quantum computers.
To realize a useful quantum computer, the quality requirements for the qubits are extremely demanding. While there are various forms of qubits today, none of them is ideal.
According to Dafei Jin, an Argonne scientist and the principal investigator of the project, an ideal qubit needs to possess at least three sterling qualities.
It needs to be able to remain in a simultaneous 0 and 1 state for a long time – scientists call this long ‘coherence’. Ideally, that time would be around a second.
Second, the qubit needs to be able to change from one state to another in a short time. Ideally, that time would be around a billionth of a second (nanosecond), the time-step of a classical computer clock.
Third, the qubit needs to be easily linked with many other qubits so they can work in parallel with each other. Scientists refer to this linking as entanglement.
Although current qubits are not ideal, companies like IBM, Intel, Google, Honeywell and many start-ups have already picked their favorite, and are aggressively pursuing technological improvement and commercialization. “Our ambitious goal is not to compete with those companies, but to discover and construct a fundamentally new qubit system that could lead to an ideal platform,” said Jin.
While there are many choices of qubit types, the team chose the simplest one – a single electron. Heating up a simple light filament can easily shoot out a boundless supply of electrons.
One of the challenges for any qubit, including an electron, is that it is very sensitive to disturbance from its surroundings. Thus, the team chose to trap an electron on an ultrapure solid neon surface in a vacuum.
Neon is one of a handful of inert elements that do not react with other elements. “Because of this inertness, solid neon can serve as the cleanest possible solid in a vacuum to host and protect any qubits from being disrupted,” said Jin.
A key component in the team’s qubit platform is a chip-scale microwave resonator made out of a superconductor (a home microwave oven is also a microwave resonator). Superconductors – metals with no electrical resistance – allow electrons and photons to interact together at near to absolute zero with minimal loss of energy or information.
“The microwave resonator crucially provides a way to read out the state of the qubit,” said Kater Murch, physics professor at the Washington University in St. Louis and a senior co-author of the paper. “It concentrates the interaction between the qubit and microwave signal. This allows us to make measurements telling how well the qubit works.”
“With this platform, we achieved, for the first time ever, strong coupling between a single electron in a near-vacuum environment and a single microwave photon in the resonator,” said Xianjing Zhou, a postdoctoral appointee at Argonne and the first author of the paper. “This opens up the possibility to use microwave photons to control each electron qubit and link many of them in a quantum processor.”
The team tested the platform in a scientific instrument called a dilution refrigerator, which can reach temperatures as low as a mere 10 millidegrees above absolute zero. This instrument is one of many quantum capabilities in Argonne’s Center for Nanoscale Materials, a DOE Office of Science user facility.
The team performed real-time operations to an electron qubit and characterized its quantum properties. These tests demonstrated that the solid neon provides a robust environment for the electron, with very low electric noise to disturb it. Most importantly, the qubit attained coherence times in the quantum state competitive with state-of-the-art qubits.
“Our qubits are actually as good as ones that people have been developing for 20 years,” said David Schuster, physics professor at the University of Chicago and a senior co-author of the paper. “This is only our first series of experiments. Our qubit platform is nowhere near optimized. We will continue improving the coherence times. And because the operation speed of this qubit platform is extremely fast, only several nanoseconds, the promise to scale it up to many entangled qubits is significant.”
There is yet one more advantage to this remarkable qubit platform. “Thanks to the relative simplicity of the electron-on-neon platform, it should lend itself to easy manufacture at low cost,” Jin said. “It would appear an ideal qubit may be on the horizon.”
This story is adapted from material from Argonne National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.