Self-driving labs like Polybot promise to streamline experimental processes, save resources and accelerate the pace of discovery. Image: Argonne National Laboratory.Researchers have a new scientific tool called Polybot that combines the power of artificial intelligence (AI) with robotics. Potential applications include speeding up the discovery of wearable biomedical devices, materials for better batteries and more.
Today’s wearable technologies like smart glasses and watches are just the start. The next generation of flexible electronics will be more efficient and sustainable, better able to monitor health and treat certain diseases, and much more. They will be composed of electronic polymer materials — a soft pliable substance that can conduct electricity.
“Just imagine the next generation of polymer electronics,” said Jie Xu, assistant chemist at the US Department of Energy (DOE)’s Argonne National Laboratory with a joint appointment in the Pritzker School of Molecular Engineering at the University of Chicago. “They are not going to be rigid anymore.”
To hasten the discovery time, researchers at Argonne have a new tool, a self-driving laboratory called Polybot that automates aspects of electronic polymer research and frees scientists’ time to work on tasks only humans can accomplish. This tool, reported in a paper in Chemistry of Materials, combines the computational power of AI with the automation possible with robotics. It is housed in the Center for Nanoscale Materials (CNM), a DOE Office of Science user facility at Argonne.
Polybot is one of several autonomous discovery labs starting up at Argonne and other research organizations. While still in their infancy, their main purpose is to harness the power of AI and robotics to streamline experimental processes, save resources and accelerate the pace of discovery.
The potential applications of Polybot extend far beyond biomedical devices, Xu said. They include developing materials for computing devices with brain-like features and new sensors for monitoring climate change. They also include developing new solid electrolytes that would eliminate the current liquid electrolytes in lithium-ion batteries, making them less likely to catch fire.
Using Polybot, the CNM team is currently focusing on polymer electronics for energy-saving and medical purposes. These include devices that are recyclable or decompose after use.
Scientists usually prepare polymers for electronics by synthesizing polymer molecules with desired chemical structures, creating a solution with a mixture of many components. They then convert this solution into a thin layer of solid material. Layers with different compositions printed together serve as the basis for making different types of devices.
To achieve targeted performance, the number of potential tweaks is overwhelming. They run from spiking the fabrication recipe with different formulations to varying the processing conditions. Using conventional experimental means, such development can take years of intense labor. Polybot can greatly reduce the development time and cost.
A typical experiment with Polybot begins by using AI and robots for different tasks. The automated system chooses a promising recipe for a polymer solution, prepares it and prints it as a very thin film at a selected speed and temperature. The system then hardens this film for an optimal length of time and measures key features, such as thickness and uniformity, as a quality check. Next, it assembles multiple layers together and adds electrodes to form a device.
After that, Polybot measures the device’s electrical performance. All the relevant data are automatically recorded and analyzed with machine learning and passed to the AI component. The AI then directs what experiments to do next. Polybot can also respond to feedback provided by users and data from the scientific literature. “This is all done with minimal human intervention,” Xu said.
“We have plans in place to expand the capabilities of our self-driving lab to take advantage of other Argonne scientific facilities,” said Henry Chan, a CNM assistant scientist.
Already, the properties of electronic devices fabricated by Polybot are analyzed with a powerful X-ray beam. This is done using an instrument with a robotic sample handler at the Advanced Photon Source (APS), a DOE Office of Science user facility at Argonne. And that connection could be strengthened to take full advantage of the APS after its upgrade is complete in 2024.
“X-ray scattering analysis expands the Polybot’s characterization down to the molecular level, revealing information about the orientation and packing of the molecules that can help speed up the search for the best materials with optimal performance,” said Joseph Strzalka, a physicist in Argonne’s X-ray Science division. “We are working on bringing the Polybot’s capabilities to an APS beamline so we can generate the large numbers of materials the APS upgrade will be capable of studying.”
“We are excited at the prospect of leveraging the supercomputing capabilities at Argonne to enhance Polybot,” Chan explained. “The goal is to conduct physics-based simulations prior to, during and after an actual experiment to gain deeper insights into a material or device and provide better feedback to the AI.” The team plans to utilize the Argonne Leadership Computing Facility, a DOE Office of Science user facility, to perform the simulations. This will streamline the discovery process even further.
With these capabilities and more, self-driving labs like Polybot have the potential to accelerate the discovery process from years to months. They also could reduce the cost of complex projects from millions to thousands of dollars.
This story is adapted from material from Argonne National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.