This new fabric being developed by University of Maryland scientists YuHuang Wang and Ouyang Min is the first textile to automatically change properties to trap or release heat depending on environmental conditions. Photo: Faye Levine, University of Maryland.Despite decades of innovation in fabrics with high-tech thermal properties that can keep marathon runners cool or alpine hikers warm, there has never been a material that changes its insulating properties in response to the environment. Until now.
Researchers at the University of Maryland (UMD) have created a fabric that can automatically regulate the amount of heat that passes through it. When conditions are warm and moist, such as those near a sweating body, the fabric allows infrared radiation (heat) to pass through. When conditions become cooler and drier, the fabric reduces the amount of heat that escapes. The fabric is described in a paper in Science.
The researchers created the fabric from specially engineered yarn coated with a conductive material. Under hot, humid conditions, the strands of yarn compact and activate the coating, which changes the way the fabric interacts with infrared radiation. The researchers refer to the action as ‘gating’ of infrared radiation, which acts as a tunable blind to transmit or block heat.
"This is the first technology that allows us to dynamically gate infrared radiation," said YuHuang Wang, a professor of chemistry and biochemistry at UMD and one of the paper's corresponding authors, who directed the studies.
The base yarn for this new textile is produced from fibers made of two different synthetic materials – one absorbs water and the other repels it – while the fibers are also coated with carbon nanotubes. Because the materials in the fibers both resist and absorb water, they warp when exposed to humidity, such as that surrounding a sweating body. That distortion brings the strands of yarn closer together, which does two things. First, it opens up pores in the fabric, which has a small cooling effect because it allows heat to escape. Second, and most importantly, it modifies the electromagnetic coupling between the carbon nanotubes in the coating.
"You can think of this coupling effect like the bending of a radio antenna to change the wavelength or frequency it resonates with," Wang said. "It's a very simplified way to think of it, but imagine bringing two antennae close together to regulate the kind of electromagnetic wave they pick up. When the fibers are brought closer together, the radiation they interact with changes. In clothing, that means the fabric interacts with the heat radiating from the human body."
Depending on the tuning, the fabric either blocks infrared radiation or allows it to pass through. The reaction is almost instant, so before people realize they're getting hot, the garment could already be cooling them down. On the flip side, as a body cools down, the dynamic gating mechanism works in reverse to trap heat.
"The human body is a perfect radiator. It gives off heat quickly," said Min Ouyang, a professor of physics at UMD and the paper's other corresponding author. "For all of history, the only way to regulate the radiator has been to take clothes off or put clothes on. But this fabric is a true bidirectional regulator."
According to the paper, this is the first textile shown to be able to regulate heat exchange with the environment.
"This pioneering work provides an exciting new switchable characteristic for comfort-adjusting clothing," said Ray Baughman, a professor of chemistry at the University of Texas who was not involved in the study. "Textiles were known that increase porosity in response to sweat or increasing temperature, as well as textiles that transmit the infrared radiation associated with body temperatures. However, no one before had found a way to switch both the porosity and infrared transparency of a textile so as to provide increased comfort in response to environmental conditions."
More work is needed before the fabric can be commercialized, but, according to the researchers, the materials used for the base fiber are readily available and the carbon coating can be easily added during a standard dyeing process.
"I think it's very exciting to be able to apply this gating phenomenon to the development of a textile that has the ability to improve the functionality of clothing and other fabrics," Ouyang said.
This story is adapted from material from the University of Maryland, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.