"In this work, we show for the first time that a superconducting qubit made from graphene is temporally quantum coherent, a key requisite for building more sophisticated quantum circuits."Joel Wang, MIT
Researchers from Massachusetts Institute of Technology (MIT) and elsewhere have recorded, for the first time, the ‘temporal coherence’ of a graphene qubit -- meaning how long it can maintain a special state that allows it to represent two logical states simultaneously. The demonstration, which used a new kind of graphene-based qubit, represents a critical step forward for practical quantum computing, the researchers say.
Superconducting quantum bits (qubits) are artificial atoms that use various methods to produce bits of quantum information, the fundamental component of quantum computers. Similar to traditional binary circuits in computers, qubits can maintain one of two states corresponding to the classic binary bits, a 0 or 1. But these qubits can also be a superposition of both states simultaneously, which could allow quantum computers to solve complex problems that are practically impossible for traditional computers.
The amount of time that these qubits stay in the superposition state is referred to as their ‘coherence time’. The longer the coherence time, the greater the ability for the qubit to compute complex problems.
Recently, researchers have been incorporating graphene-based materials into superconducting quantum computing devices, which promise faster, more efficient computing, among other perks. Until now, though, there's been no recorded coherence for these advanced graphene qubits, so there's no knowing if they're feasible for practical quantum computing.
In a paper in Nature Nanotechnology, the researchers report, for the first time, a coherent qubit made from graphene and exotic materials. These materials allow the qubit to change states through voltage, much like transistors in today's traditional computer chips – and unlike most other types of superconducting qubits. Moreover, the researchers could put a number on the coherence, clocking it at 55 nanoseconds, before the qubit returns to its ground state.
The work combined expertise from co-authors William Oliver, a physics professor at MIT whose work focuses on quantum computing systems, and Pablo Jarillo-Herrero, another physics professor at MIT, who researches innovations in graphene.
"Our motivation is to use the unique properties of graphene to improve the performance of superconducting qubits," explains first author Joel Wang, a postdoc in Oliver's group in the Research Laboratory of Electronics (RLE) at MIT. "In this work, we show for the first time that a superconducting qubit made from graphene is temporally quantum coherent, a key requisite for building more sophisticated quantum circuits. Ours is the first device to show a measurable coherence time – a primary metric of a qubit – that's long enough for humans to control."
There are 14 other co-authors of the paper. They include: Daniel Rodan-Legrain, a graduate student in Jarillo-Herrero's group who contributed equally to the work with Wang; MIT researchers from RLE, the Department of Physics, the Department of Electrical Engineering and Computer Science, and Lincoln Laboratory; and researchers from the Laboratory of Irradiated Solids at the École Polytechnique, CNRS in France and the Advanced Materials Laboratory of the National Institute for Materials Science in Japan.
Superconducting qubits rely on a structure known as a ‘Josephson junction’, where an insulator (usually an oxide) is sandwiched between two superconducting materials (usually aluminum). In traditional tunable qubit designs, a current loop creates a small magnetic field that causes electrons to hop back and forth between the superconducting materials, causing the qubit to switch states. But this flowing current consumes a lot of energy and causes other issues.
Recently, a few research groups have tried replacing the insulator with graphene, an atom-thick layer of carbon that's inexpensive to mass produce and has unique properties that might produce faster, more efficient computation.
To fabricate their qubit, the researchers turned to a class of materials called van der Waals materials – atom-thin materials that can be stacked like Lego bricks on top of one another, with little to no resistance or damage. These materials can be stacked in specific ways to create various electronic systems. Despite their near-flawless surface quality, only a few research groups have ever applied van der Waals materials to quantum circuits, and none of these materials have previously been shown to exhibit temporal coherence.
For their Josephson junction, the researchers sandwiched a sheet of graphene between two layers of a van der Waals insulator called hexagonal boron nitride (hBN). Importantly, graphene takes on the superconductivity of the superconducting materials it touches. The selected van der Waals materials can be made to usher electrons around using voltage, instead of the traditional current-based magnetic field. Therefore, so can the graphene – and so can the entire qubit.
When voltage gets applied to the qubit, electrons bounce back and forth between two superconducting leads connected by graphene, changing the qubit from ground (0) to an excited or superposition state (1). The bottom hBN layer serves as a substrate to host the graphene, while the top hBN layer encapsulates the graphene, protecting it from any contamination. Because the materials are so pristine, the traveling electrons never interact with defects. This represents the ideal ‘ballistic transport’ for qubits, where a majority of electrons move from one superconducting lead to another without any scattering from impurities, making a quick, precise change of states.
This work can help tackle the qubit ‘scaling problem’, Wang says. Currently, only about 1000 qubits can fit on a single chip. Having qubits controlled by voltage will be especially important as millions of qubits start being crammed on a single chip. "Without voltage control, you'll also need thousands or millions of current loops too, and that takes up a lot of space and leads to energy dissipation," he explains.
Additionally, voltage control means greater efficiency and a more localized, precise targeting of individual qubits on a chip, without ‘cross talk’. That happens when a little bit of the magnetic field created by the current interferes with a qubit it's not targeting, causing computation problems.
For now, the researchers' qubit has a brief lifetime. For reference, conventional superconducting qubits that hold promise for practical application have documented coherence times of a few tens of microseconds, a few hundred times greater than the researchers' qubit.
But the researchers are already addressing several issues that cause this short lifetime, most of which merely require structural modifications. They're also using their new coherence-probing method to further investigate how electrons move ballistically around the qubits, with aims of extending the coherence of qubits in general.
This story is adapted from material from MIT, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.