This figure shows a comparison of the activation energies involved in the autocatalytic surface reduction for the growth of palladium nanocrystals. Image: Xia laboratory, Georgia Tech.Researchers at Georgia Institute of Technology have published the first part of what they expect to be a database showing the kinetics involved in producing colloidal metal nanocrystals via an autocatalytic process. Such nanocrystals are suitable for catalytic, biomedical, photonic and electronic applications.
In the solution-based process, precursor chemicals adsorb to nanocrystal seeds before being reduced to atoms that fuel growth of the nanocrystals. The researchers produced the kinetics data by conducting painstaking systematic studies to determine growth rates on different nanocrystal facets – surface structures that control how the crystals grow by attracting individual atoms.
In a paper published in the Proceedings of the National Academy of Sciences, the Georgia Tech research team provided a quantitative picture of how surface conditions control the growth of palladium nanocrystals. The work, which will later include information on nanocrystals made from other noble metals, is supported by the US National Science Foundation.
"This is a fundamental study of how catalytic nanocrystals grow from tiny seeds, and a lot of people working in this field could benefit from the systematic, quantitative information we have developed," said Younan Xia, professor in the Department of Biomedical Engineering at Georgia Tech and Emory University. "We expect that this work will help researchers control the morphology of nanocrystals that are needed for many different applications."
A critical factor controlling how nanocrystals grow from tiny seeds is the surface energy of the crystalline facets on the seeds. Researchers have known that energy barriers dictate the surface attraction for precursors in solution, but specific information on the energy barrier for each type of facet had not been readily available.
"Typically, the surface of the seeds that are used to grow these nanocrystals has not been homogenous," explained Xia, who is also the Georgia Research Alliance eminent scholar in nanomedicine and holds joint appointments in the School of Chemistry & Biochemistry and the School of Chemical & Biomolecular Engineering. "You may have different facets on the crystals, which depend on the arrangement of the atoms below them. From the standpoint of precursors in the solution around the seeds, these surfaces have different activation energies which determine how difficult it will be for the precursors or atoms to land on each surface."
Xia's research team designed experiments to assess the energy barriers on various facets, using seeds of a variety of sizes and surface configurations chosen to have only one type of facet. The researchers measured both the growth of the nanocrystals in solution and the change in the concentration of the palladium tetrabromide (PdBr42-) precursor salt.
"By choosing the right precursor, we can ensure that all the reduction we measure is on the surface and not in the solution," Xia said. "That allowed us to make meaningful measurements about the growth, which is controlled by the type of facet, as well as presence of a twin boundary, corresponding to distinctive growth patterns and end results."
Over the course of nearly a year, visiting graduate research assistant Tung-Han Yang studied nanocrystal growth using different types of seeds. Rather than allowing nanocrystal growth from self-nucleation, Xia's team chose to study growth from seeds so they could control the initial conditions.
Controlling the shape of the nanocrystals is critical to applications in catalysis, photonics, electronics and medicine. Because these noble metals are expensive, minimizing the amount of material needed for catalytic applications helps control costs.
"When you do catalysis with these materials, you want to make sure the nanocrystals are as small as possible and that all of the atoms are exposed to the surface," said Xia. "If they are not on the surface, they won't contribute to the activity and therefore will be wasted."
The ultimate goal of the research is a database that scientists can use to guide the growth of nanocrystals with specific sizes, shapes and catalytic activity. Beyond palladium, the researchers plan to publish the results of similar kinetic studies for gold, silver, platinum, rhodium and other nanocrystals. While the pattern of energy barriers will likely be different for each metal nanocrystal, there will be similarities in how the energy barriers control growth, Xia said.
"It's really how the atoms are arranged on the surface that determines the surface energy," he explained. "Depending on the metals involved, the exact numbers will be different, but the ratios between the facet types should be more or less the same."
Xia hopes that the work of his research team will lead to a better understanding of how the autocatalytic process works in the synthesis of these nanomaterials, and ultimately to broader applications.
"If you want to control the morphology and properties, you need this information so you can choose the right precursor and reducing agent," said Xia. "This systematic study will lead to a database on these materials. This is just the beginning of what we plan to do."
This story is adapted from material from Georgia Institute of Technology, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.