Researchers have found a new approach for reducing the number of loops (red) in a polymer. This method could offer an easy way for manufacturers of industrially-useful materials such as plastics or gels to strengthen their materials. Image courtesy of the researchers.Plastic, rubber and many other useful materials are made of polymers – long chains arranged in a cross-linked network. But at the molecular level, these polymer networks can contain structural flaws that weaken them.
Several years ago, researchers at Massachusetts Institute of Technology (MIT) were the first to measure certain types of these defects, called ‘loops’, which occur when a chain in the polymer network binds to itself instead of another chain. Now, the same researchers, together with colleagues at Case Western Reserve University, have found a simple way to reduce the number of loops in a polymer network and thus strengthen materials made from polymers.
To achieve this, the researchers simply add one of the components of the polymer network very slowly to a large quantity of the second component. Using this approach, they were able to cut the number of loops in half, in a variety of different polymer network structures. This could offer an easy way for manufacturers of industrially-useful materials such as plastics or gels to strengthen their materials.
"Just by changing how fast you add one component to the other, you can improve the mechanical properties," says Jeremiah Johnson, an associate professor of chemistry at MIT and senior author of a paper on this work in the Proceedings of the National Academy of Sciences.
In 2012, Johnson's group devised the first way to measure the number of loops in a polymer network and validated those results with theoretical predictions from Bradley Olsen, an associate professor of chemical engineering at MIT. The researchers found that loops can comprise from around 9% to nearly 100% of the network, depending on the concentration of polymer chains in the starting material and other factors.
A few years later, Johnson and Olsen developed a way to calculate how much these loops weaken a material. In their latest work, they set out to reduce loop formation, and to achieve this without changing the composition of the materials.
"The goal we set for ourselves was to take the same set of precursors for a material that one would normally use, and, using the exact same precursors under the same conditions and at the same concentration, make a material with fewer loops," Johnson says.
The researchers first focused on a type of polymer structure known as a star polymer network. This material has two different building blocks: a star with four identical arms, known as ‘B4’, and a chain known as ‘A2’. Each molecule of A2 attaches to the end of one of the B4 arms. However, during a typical synthesis process, when everything is mixed together at once, some of the A2 chains end up binding to two of the B4 arms, forming a loop.
The researchers found, however, that if they added B4 very slowly to a solution of A2, each of the B4 arms would quickly react with a single molecule of A2, so there was less opportunity for A2 to form loops.
After a few hours of slowly adding half of the B4 solution, they added the second half all at once, and the star-shaped subunits joined together to form a cross-linked network. This material, the researchers found, had about half as many loops as the same material produced using the traditional synthesis process. Depending on how many loops were in the original material, this ‘slow then fast’ strategy can improve the material's strength by as much as 600%, Johnson says.
The researchers also tried this technique with four other types of polymer network synthesis reactions. They were not able to measure the number of loops for all these types of polymers, but they did find similar improvements in the strength of the materials.
This approach could potentially help to improve the strength of any material made from a gel or other cross-linked polymer, including plastics, membranes for water purification, adhesives made of epoxy or hydrogels such as contact lenses. Johnson's lab is now working on applying this strategy to a variety of materials, including gels used to grow cells for tissue engineering.
This story is adapted from material from MIT, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.