Technologies for removing carbon from the atmosphere keep improving, but solutions for what to do with the carbon once it’s been captured are harder to come by.
Together with collaborators, the lab of Pulickel Ajayan, a materials scientist at Rice University, has now developed a way to wrest the carbon from carbon dioxide and affix it to hydrogen atoms, forming methane ? a valuable fuel and industrial feedstock. As reported in a paper in Advanced Materials, their method relies on electrolysis with catalysts developed by grafting isolated copper atoms onto two-dimensional (2D) polymer templates.
“Electricity-driven carbon dioxide conversion can produce a large array of industrial fuels and feedstocks via different pathways,” said Soumyabrata Roy, a research scientist in the Ajayan lab and the paper’s lead author. “However, carbon dioxide-to-methane conversion involves an eight-step pathway that raises significant challenges for selective and energy-efficient methane production.
“Overcoming such issues can help close the artificial carbon cycle at meaningful scales, and the development of efficient and affordable catalysts is a key step toward achieving this goal.”
The 2D polymer templates, made of alternating carbon and nitrogen atoms, have tiny pores where copper atoms can fit at varying distances from one another. The catalysts assemble at room temperature in water, with the copper atoms displacing the host metal ions in the polymer templates. When tested in a reactor, the catalysts promoted the reduction of carbon dioxide to methane in one half of the cell, while oxygen was produced from water in the other half.
“We found that modulating the distances between the copper atoms lowered the energy needed for key reaction steps, thereby speeding up the chemical conversion,” Roy said. “This cooperative action of nearby copper atoms helped produce methane at a very high rate of selectivity and efficiency.”
The catalysts developed by Roy and his collaborators yielded one of the most rapid and efficient electrolysis-based conversions of carbon dioxide to methane known to date, helping advance the conversion process both in terms of fundamental scientific insight and performance level.
“If system-level energy and carbon conversion efficiencies can be addressed, inexpensive and efficient materials like these will help catalyze the industrial translation of electrochemical carbon dioxide reduction technology,” said Jingjie Wu, an associate professor of chemical and environmental engineering at the University of Cincinnati and a co-author of the paper.
Ajayan, who is professor of engineering and chair of the Department of Materials Science and NanoEngineering, added that the “design and development of novel catalysts are central to the energy and sustainability challenges we face. Single-atom-dispersed catalysts present an exciting approach in this effort.”
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.