Materials scientists led by a team at the US Department of Energy's Pacific Northwest National Laboratory (PNNL) have designed a tiny tube that rolls up and zips closed. These hollow nanotubes are thousands of times smaller than a strand of human hair and could help with water filtration, tissue engineering and many other applications.
The tubes were inspired by protein structures called microtubules that reside in cells, according to PNNL's Chun-Long Chen. "The structure of the cell is so beautiful," said Chen, a materials chemist who conceived of and directed this project. "We wanted to create a synthetic system that mimics the microtubule structure and is stable enough for a variety of technical applications." Chen, his PNNL colleagues and their collaborators report the project in a paper in Nature Communications.
Microtubules are tiny hollow tubes that help keep DNA organized during cell division and form highways for shuttling contents around the cell. These cellular roads are composed of long chains of proteins that come together into a rigid, but hollow, tube. Microtubules have a uniform but dynamic structure, and they inspire scientists like Chen.
Chen's group hopes to use tiny hollow tubes like microtubules to create a robust water filtration system that would capture salt or other molecules within the tubes and let pure water escape out the other end. In addition, they want to monitor how stem cells adapt to different environments by studying how the cells change while they grow on these tubes.
But the researchers can't use microtubules themselves for these projects. Microtubules may be rigid and responsive, but they're also susceptible to temperature changes and microbes. "If we want to use microtubules for water filtration, you don't want to have a filter that can be eaten by bacteria," said Chen.
So the team set about making a synthetic version of microtubules using protein-like molecules called peptoids. Like proteins, peptoids are composed of a repeating pattern of building blocks with slight variations, but peptoids are more stable.
These new nanotubes form in a unique way. First, small peptoid particles come together to form a sheet, which then closes at one end and rolls into a seamless tube. To characterize the nanotubes, the scientists used a variety of techniques, including some at the Advanced Light Source and the Molecular Foundry, two DOE Office of Science User Facilities at Lawrence Berkeley National Laboratory.
Chen and his team discovered that these nanotubes are highly tailorable. The group could control a tube's size, diameter, thickness and stiffness by adjusting the tube composition or changing the acidity of the solution.
To test the rigidity of the nanotubes, Chen's team applied pressure to individual nanotubes and measured how they changed shape. The tubes have a rigidity that falls between biological tissue and harder substances like glass and mica, which, said Chen, is great for the types of experiments he hopes to do.
But Chen doesn't want to stop there. For him, the goal is to create something that mimics nature in structure and function. "Nature has offered us all kinds of beautiful examples," he said. "Fish can take in water from the sea without having to worry about high salt conditions. If we could mimic this behavior by building artificial cell membranes containing these nanotubes, we could solve some of the big problems facing our world today."
This story is adapted from material from Pacific Northwest National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.
Scientists at PNNL have created a new family of nanotubes composed of protein-like molecules called peptoids. As the diagrams show, these nanotubes start out as small droplets that come together to form a cell-membrane-like sheet, which then folds at one end and zips closed into a tube. Image: PNNL.