Amorphous CHANGE TOPIC

Amorphous materials news, June 2022

Taking steps towards new carbon structures

well-ordered novel carbon nanostructures such as nanowalls can be grown by electrodeposition from molten salts

Surface modification makes carbon fiber composites tougher

electrochemical modification of carbon fibers makes polymer composites tougher

Using computer modelling, researchers have predicted the existence of a new layered form of carbon they call 'amorphous graphite'.

Scientists used sophisticated molecular dynamics simulations to better understand the unusual properties of amorphous materials such as glass.

Researchers have developed an oxysulfide glass electrolyte for use in ambient-temperature solid-state sodium-sulfur batteries.

green-solvent-processable, open-air printable self-assembly strategy for fabricating stable, efficient OSCs

News archive…

Connect with us
Most viewed in amorphous materials…
News
 

new scaffold material support bone regeneration and regrowth, while reducing chance of infection

News
 

self-sensing, self-healing composite could extend the life of composites used in transport and renewable energy applications

Current research