Current research
Volume 61, Pages 22–29Jianxin Cao, Xiaoye Luo, Shilian Yang, Fei Liu, Peng Chen, Shuang-Feng Yin
News
self-sensing, self-healing composite could extend the life of composites used in transport and renewable energy applications
30 January 2023Cordelia Sealy
Current research
Volume 61, Pages 11–21Q. Chao, X.Y. Cui, Z.B. Chen, A.J. Breen, M. Cabral, N. Haghdadi, Q.W. Huang, R.M. Niu, H.S. Chen, B. Lim, S. Primig, M. Brandt, W. Xu, S.P. Ringer, X.Z. Liao