Cookies enable us to provide the best experience possible and help us understand how visitors use our website. By browsing Materials Today, you agree to our use of cookies.
An artificial intelligence system has discovered three new metallic glass materials 200 times faster than could be done before.
Scientists have furthered their understanding of how, when and where the atoms in molten metal ‘lock’ into place during the production of metallic glass.