Composites CHANGE TOPIC

Composites news, October 2023

Researchers have combined metal nanoclusters and graphene nanosheets to produce a new and imporved separator for lithium-sulfur batteries.

News archive…

Connect with us
Most viewed in composites…
Current research
 

News
 

Addition of titanium carbide-based materials significantly reduces friction and wear

Current research
 
News
 

By combining chitosan from crabs and agarose from seaweed, researchers created biopolymer composite films with enhanced strength.

News
 

Researchers have developed a new polymer composite that can change its behavior depending on temperature to perform specific tasks.