Using an advanced imaging technique, researchers have mapped, for the first time ever, the 3D atomic coordinates of medium- and high-entropy alloys.

A novel superconducting material is uniquely sensitive to outside stimuli, allowing its superconducting properties to be enhanced or suppressed at will.

A 3D model created by AI helped researchers to understand the formation of dislocations in complex polycrystalline materials.

Using lasers, researchers have managed to observe the ballistic movement of electrons in graphene in real time.

Researchers have demonstrated that the magnetic moment of chiral phonons is significantly enhanced in topological materials.

Researchers have combined two nanosized crystalline materials onto a single chip and shown that one can efficienctly transmit light to the other.

Researchers have shown that acoustic emissions can be used to detect defects during the laser additive manufacturing of metallic objects.

Using diamond quantum magnetometry. researchers have, for the first time, detected magnetic monopoles in a material closely related to rust.

By mapping the structural features of a 2D ferroelectric material, researchers have revealed how domains in the material impact its behavior.

Researchers have used piezoelectric nanoparticles to investigate the physical forces at play in non-Newtonian fluids.

Even at large scales, the amount of friction between two silicon surfaces is determined by microscopic chemical bonds between them.

News archive…

Connect with us
Most viewed in characterization…
Feature
 

Current research
 
News
 

Using an advanced imaging technique, researchers have mapped, for the first time ever, the 3D atomic coordinates of medium- and high-entropy alloys.

Review
 

Current research