A polymer gel that incorporates chloroplasts from plants can react with carbon dioxide in the air to grow, strengthen and even repair itself.

Australian researchers combine titanium dioxide and graphene to develop a novel, low-power sun sensor.

By creating nanoporous graphene and then covering it with a polymer layer, engineers have fabricated an atomically thin membrane.

Engineers have developed a graphene-based technique for fabricating ultrathin, flexible semiconducting films from exotic materials.

graphdiyne film filters lithium ions and prevents dendrite growth in lithium-metal batteries

Non-precious metal Fe-N doped carbon electrocatalyst for ORR could make fuel cells more economically viable and sustainable.

Physicists have developed a bilayer graphene device that displays both efficient transport and control of electron spins.

manganese selenide nanocubes are promising anode materials for sodium-ion batteries

Acid-resistant CNT-supported iridium-oxide catalyst for oxygen evolution and reduction reactions.