Researchers have shown that an alloy of nickel and gold displays particularly promising thermoelectric properties.
19 September 2023
Researchers have shown that conerting waste plastics into graphene by rapid flash Joule heating also results in the production of hydrogen.
18 September 2023
New material makes data encryption safer
15 September 2023Laurie Donaldson
By mining data from X-ray images, researchers have made significant new discoveries about the reactivity of lithium iron phosphate electrodes.
14 September 2023
Rechargeable battery with improved operating voltage and energy density
11 September 2023Laurie Donaldson
Researchers have discovered a previously unknown reaction pathway that could addresses the short lifetimes of lithium-sulfur batteries.
5 September 2023
Researchers have developed a novel catalyst for reducing carbon dioxide by loading silver nanoparticles onto a titanium dioxide support.
4 September 2023