Scientists have developed a way to integrate transparent conducting metal oxide contacts with 2D semiconductors to produce see-through electronic devices.

For the first time, scientists have observed ion migration within hybrid perovskite crystals and related that to declines in its light-absorbing ability.

A novel method for synthesizing nanoparticles of europium(II) oxide is allowing scientists to study the properties of this ferromagnetic semiconductor.

Researchers have managed to control the fluorescence emitted by carbon nanotubes by attaching hexagonal carbon molecules to them.

Borophene could be the first pure two-dimensional material able to emit visible and near-infrared light by activating its plasmons.

Researchers have created the material for a chemical heat 'battery' that can release its energy on demand.

The optical and photocatalytic properties of carbon dots can be precisely tuned by controlling the positions of nitrogen atoms in their structure.

News archive…

Connect with us
Most viewed in optical materials…
Current research
 

Current research
 

Current research
 

Current research
 

Current research
 

What’s coming up in optical materials…
24
Oct ’22