Researchers have developed an organic cathode that dramatically improves the stability and energy density of solid-state sodium-ion batteries.

Researchers have shown that a nano-coating of boron nitride can stabilize solid electrolytes in lithium metal batteries.

Researchers have discovered why vanadium disulfide is unstable as a battery cathode material and developed a way to make it more stable.

High-quality phosphorene nanoribbons for high-speed electronics

Researchers have improved the optical properties of the 2D material molybdenum disulphide by removing defects with laser light and water.

Scientists have theorized a new ‘oil-and-vinegar’ approach for inducing spherical nanoparticles to self-assemble into unusual architectures.